Alkali-free glass and method for producing same
Abstract
The present invention provides an alkali-free glass having a high strain point, a low viscosity and low devitrification, which is easily subjected to float molding and fusion molding. The glass herein has a strain point of 725° C. or higher, an average thermal expansion coefficient at 50 to 300° C. of 30×10 −7 to 40×10 −7 /° C., a temperature T 2 at which a glass viscosity becomes 10 2 dPa·s of 1,710° C. or lower, a temperature T 4 at which a glass viscosity becomes 10 4 dPa·s of 1,330° C. or lower, a glass surface devitrification temperature (T c ) of 1,330° C. or lower, and a glass internal devitrification temperature (T d ) of 1,330° C. or lower.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 11.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An alkali-free glass, comprising, in terms of mol % on the basis of oxides: SiO 2 : 66 to 70; Al 2 O 3 : 12 to 13.5; B 2 O 3 : 0.7 to 1.5; MgO: 6 to 9.5; CaO: 4.5 to 6; SrO: 4 to 7; BaO: 0 to less than 1; and ZrO 2 : 0 to 0.5, provided that: MgO+CaO+SrO+BaO is 14 to 18.2; MgO/(MgO+CaO+SrO+BaO) is 0.35 or greater; MgO/(MgO+CaO) is 0.52 or greater; and MgO/(MgO+SrO) is 0.45 or greater, wherein the alkali-free glass does not substantially contain alkali metal oxides, and has the following characteristics: a strain point of 725° C. or higher; an average thermal expansion coefficient at 50 to 300°
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (11 of 11 total)
References Cited — Backward Prior Art (18)
Non-Patent Literature (2)
- International Search Report issued Aug. 17, 2010 in PCT/JP2010/060904 filed Jun. 25, 2010.
- Machine Translation of JP 10-045422 A, Feb. 17, 1998.