Non-alkali glass, and process for production of non-alkali glass
Abstract
The present invention relates to an alkali-free glass having a strain point of 735° C. or higher, an average thermal expansion coefficient at from 50 to 350° C. of from 30×10 −7 to 40×10 −7 /° C., a temperature T 2 at which a glass viscosity is 10 2 dPa·s of 1,710° C. or lower, a temperature T 4 at which a glass viscosity is 10 4 dPa·s of 1,340° C. or lower, and a devitrification temperature of 1,330° C. or lower, the alkali-free glass including, in terms of mol % on the basis of oxides: SiO 2 66 to 69, Al 2 O 3 12 to 15, B 2 O 3 0 to 1.5, MgO 6 to 9.5, CaO 7 to 9, SrO 0.5 to 3, BaO 0 to 1, and ZrO 2 0 to 2, in which MgO+CaO+SrO+BaO is from 16 to 18.2, MgO/(MgO+CaO+SrO+BaO) is 0.35 or more, MgO/(MgO+CaO) is 0.40 or more and less than 0.52, and MgO/(MgO+SrO) is 0.45 or more.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An alkali-free glass comprising, in terms of mol % on the basis of oxides: SiO 2 66 to 69, Al 2 O 3 12 to 15, B 2 O 3 0 to 1.5, MgO 6 to 9.5, CaO 7 to 9, SrO 0.5 to 3,
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (16)
Non-Patent Literature (4)
- Extended European Search Report issued on Jun. 23, 2014 in the corresponding European Application No. 11852770.4.
- International Search Report issued Feb. 7, 2012 in PCT/JP2011/079479 filed Dec. 20, 2011.
- U.S. Appl. No. 13/912,642, filed Jun. 7, 2013, Tsujimura, et al.
- U.S. Appl. No. 14/048,382, filed Oct. 8, 2013, Tsujimura, et al.