Disclosed is alkali-free glass which has high strain point, low viscosity and low devitrification properties, and which can be easily formed by float forming or fusion forming. The alkali-free glass has a strain point of not less than 725˚C, an average thermal expansion…
Tsujimura Tomoyuki
The present invention relates to an alkali free glass in which the strain point is 725°C or more, the average thermal expansion coefficient at 50-300°C is 3x10 -7 -40x10 -7 /°C, the temperature (T 2 ) at which glass viscosity becomes 10 2 dPa·s is 1710°C or less, and the…
The present invention provides an alkali-free glass having a high strain point, a low viscosity and low devitrification, which is easily subjected to float molding and fusion molding. The glass herein has a strain point of 725° C. or higher, an average thermal expansion…
A process for glass production in which a reduction in melting temperature in producing a molten glass from a raw glass material can be attained to reduce energy consumption and glass composition homogenization can also be attained. Also provided are: a process for producing a…
A process for glass production which attains a reduction in energy consumption and can produce a homogeneous glass product of high quality which is extremely reduced in bubble inclusion and contains no particles resulting from an unmelted raw material. The process for glass…
Disclosed is a method for producing a non-alkaline glass having little bubbles therein and excellent in homogeneity and flatness. Specifically disclosed is a method for producing a non-alkaline glass, which comprises melting a glass raw material containing a silicon source and…
Disclosed is a glass plate for a substrate, which contains little B 2 O 3 and has a β-OH value (mm -1 ) of 0.05-0.5. The glass plate for a substrate is suitable for use as a glass plate for a TFT panel. Specifically disclosed is a glass plate for a substrate, which has a glass…
The present invention provides an alkali-free glass having a high strain point, a low viscosity and low devitrification, which is easily subjected to float molding and fusion molding. The glass herein has a strain point of 725° C. or higher, an average thermal expansion…
The present invention relates to a non-alkali glass which has a strain point of 735˚C or higher, an average thermal expansion coefficient of 30×10 -7 to 40×10 -7 /˚C at 50 to 350˚C, a temperature (T 2 ) at which the viscosity of the glass becomes 10 2 dPa·s of 1710˚C or lower, a…
The present invention relates to a glass plate for a substrate contains, as a glass matrix composition, in mol % on the oxide basis, SiO 2 : 67 to 72, Al 2 O 3 : 1 to 7, B 2 O 3 : 0 to 4, MgO: 11 to 15, CaO: 0 to 3, SrO: 0 to 3, BaO: 0 to 4, ZrO 2 : 0 to 4, Na 2 O: 8 to 15, and…
The present invention pertains to: a method for producing a lithium-ion conductive solid electrolyte to be used in lithium-ion secondary batteries and the like; and a lithium-ion secondary battery having such a lithium-ion conductive solid electrolyte. In the prior art, methods…
The objective of the present invention is to provide a glass with a high bubble quality having less bubbles. The present invention relates to a method for melting glass material in which glass material particles produced by granulating a glass material containing a plurality of…
The present invention pertains to: a lithium-ion conductive glass ceramic to be used in lithium-ion secondary batteries and the like; and a method for producing the lithium-ion conductive glass ceramic. The inorganic solid electrolytes of the prior art have problems such as…
Disclosed is a method for producing a highly uniform and highly flat alkali-free glass which has only a few bubbles therein. Specifically disclosed is a method for producing an alkali-free glass, wherein a glass raw material containing a silicon source, an alkaline earth metal…
According to the present invention, a non-alkali glass for substrates which has a sheet thickness of 0.1 to 0.3mm and a compaction of 9ppm or less can be obtained without subjecting a non-alkali glass for substrates after manufacturing (after forming, annealing and cutting) to…
The present invention relates to a glass plate for a substrate contains, as a glass matrix composition, in mol % on the oxide basis, SiO 2 : 67 to 72, Al 2 O 3 : 1 to 7, B 2 O 3 : 0 to 4, MgO: 11 to 15, CaO: 0 to 3, SrO: 0 to 3, BaO: 0 to 4, ZrO 2 : 0 to 4, Na 2 O: 8 to 15, and…
To provide a method whereby it is possible to produce an alkali-free glass having little bubbles therein and excellent in homogeneity and flatness. A method for producing an alkali-free glass, which comprises melting a glass raw material containing a silicon source, followed by…