Non-alkali glass substrate
Abstract
The present invention relates to a non-alkali glass substrate, having a strain point of 685° C. or higher and 750° C. or lower, an average thermal expansion coefficient at 50 to 350° C. of from 35×10 −7 to 43×10 −7 /° C., a specific gravity of from 2.50 to 2.80, a photoelastic constant of 25 nm/MPa/cm or more and less than 29 nm/MPa/cm, and a temperature (T 4 ) at which viscosity reaches 10 4 dPa·s of 1,250° C. or higher and lower than 1,350° C., and having a prescribed composition.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 6.
Claims (3 — 3 Independent, 0 Dependent)
- Claim 1Independent Claim
A non-alkali glass substrate, having a strain point of 685° C. or higher and 750° C. or lower, an average thermal expansion coefficient at 50 to 350° C. of from 35×10 −7 to 43×10 −7 /° C., a specific gravity of from 2.50 to 2.80, a photoelastic constant of 25 nm/MPa/cm or more and less than 29 nm/MPa/cm, and a temperature (T 4 ) at which viscosity reaches 10 4 dPa·s of 1,250° C. or higher and lower than 1,350° C., and comprising, indicated by mol % on the basis of oxides, 63% or more and 68% or less of SiO 2 ,
- Claim 6Independent Claim
5% or more and 13% or less of MgO, 0% or more and less than 4% of CaO, 0% or more and 9% or less of SrO, and 0% or more and 10% or less of BaO, wherein MgO+CaO+SrO+BaO is from 15 to 20%, and SrO+BaO is from 4 to 10%.
- Claim 12Independent Claim
2% or more and 14% or less of Al 2 O 3 , 0.5% or more and less than 3% of B 2 O 3 ,
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (29)
Non-Patent Literature (2)
- International Search Report issued Mar. 11, 2014 in PCT/JP2013/082365 filed Dec. 2, 2013.
- Machine translation of JP 09-263421, Oct. 7, 1997.