Polyester fiber and process for producing the same
Abstract
A polyester fiber and process embodiments for the production thereof are described, wherein the polyester fiber is produced by high-speed spinning and is characterized by a filament fineness of from 1 to 3 d, a strength of at least 4.0 g/d, an elongation of up to 40%, a crystallinity (Xρ) of from 40 to 55%, a birefringence of from 140×10 -3 to 165×10 -3 , an orientation function of from 0.36 to 0.45 in the amorphous portion, and a thermal shrinking stress that satisfies the relations 1.1≦ST.sub.200 /ST.sub.100 ≦2.0 (I) and 50≦ST.sub.max ≦180 (II), where ST 100 is the shrinking stress (mg/d) at 100° C., ST 200 is the shrinking stress (mg/d) at 200° C., and ST max is a peak stress (mg/d) on a thermal shrinking stress curve.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 18.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A polyester fiber produced by high-speed spinning which is characterized by a filament fineness of from 1 to 3 d, a strength of at least 4.0 g/d, an elongation of up to 40%, a crystallinity (Xρ) of from 40 to 55%, a birefringence of from 140×10 -3 to 165×10 -3 , an orientation function of from 0.36 to 0.45 in the amorphous portion, and a thermal shrinking stress that satisfies the relations 1.1≦ST.sub.200 /ST.sub.100 ≦2.0 (I) and 50≦ST.sub.max ≦180 (II), where ST 100 is the shrinking stress (mg/d) at 100° C., ST 200 is the shrinking stres
- Claim 2Depends on #1
A polyester fiber according to claim 1, wherein the strength is at least 4.2 g/d, the elongation is up to 35%, and the birefringence is from 145
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗