Patents
US 4,156,071 A#392646 Most CitedExpiredUnited States (USPTO)Utility

Poly(ethylene terephthalate) flat yarns and tows

78Forward Citations (#392646 Global)
1.7/yrCitation Velocity (#2968504 Global)
17.31Citation PageRank (#425188 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

New poly(ethylene terephthalate) flat yarns and tows having physical properties and dyeability more akin to cellulose acetate than to conventional poly(ethylene terephthalate) flat yarns are prepared directly by spinning at speeds of about 4000 meters/minute. Among the useful physical properties are a modulus of 30 to 65, which is relatively unaffected by boiling, low boil-off shrinkage, no need for heat setting, low shrinkage tension, large crystal size, and low amorphous orientation which is measured by a value termed "amorphous modulus." The flat yarns may be used, e.g. in textile fabrics, without drawing, and may be modified, e.g. by air-jet texturing. The tows may be converted into staple fiber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 78.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A flat yarn comprising continuous filaments of poly(ethylene terephthalate) of 1 to 7 denier per filament, and intrinsic viscosity [η] 0.56 to 0.68, characterized by: (1) a relative disperse dye rate of at least 0.09, (2) a modulus of about 30 to about 65 grams/denier, when measured on the yarn as-produced (M) and after being boiled in water at atmospheric pressure for 60 minutes (M 2 ), (3) an amorphous modulus (M A ) of from about 28 to about 38 grams/denier, where the amorphous moduus is related to the modulus (M), the intrinsic viscosity [η] and the density of the poly(ethylene terepht

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗