Patents
US 4,134,882 A#169554 Most CitedExpiredUnited States (USPTO)Utility

Poly(ethylene terephthalate)filaments

117Forward Citations (#169554 Global)
2.5/yrCitation Velocity (#1347841 Global)
30.45Citation PageRank (#164771 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Poly(ethylene terephthalate) filaments of enhanced dyeability, low boil-off shrinkage (even in as-spun condition), good thermal stability over a large temperature range, and useful as texturing feed yarns and/or as hard yarns requiring no further drawing are prepared by spinning at extremely high speeds, and are characterized by a long period spacing above 300 A in their as-spun condition, and, whether in as-spun condition or after heat-treatment, by a low skin-core value as measured by a differential birefringence in relation to their stress measured at 20% extension (which correlates approximately with the spinning speed), a large crystal size, and low amorphous orientation. The continuous filament yarns may be draw-textured to provide textured yarns which also show enhanced dyeability. The staple fiber yarns also have very useful properties as compared with conventional staple yarns. A preferred process of spinning at these extremely high speeds is characterized by the use of a spinneret with capillary-dimensions that produce high shear as the polyester is extruded, and is applicable also to copolyesters, whose filaments show a similar low skin-core in relation to their stress a

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 117.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Poly(ethylene terephthalate) filaments of enhanced dyeability and low shrinkage, characterized by a long-period spacing of more than 300 A and by a differential birefringence (Δ 95-5 ) between the surface and the core of the filament of less than about 0.0055 + 0.0014 δ 20 , where δ 20 is the stress measured at 20% extension, and is at least about 1.6 gpd.

  2. Claim 2Depends on #1

    A hard yarn comprising filaments according to claim 1, wherein δ 20 is at least about 2.6 gpd.

  3. Claim 3Depends on #1

    A yarn comprising filaments according to claim 1, whose boil-off shrinkage is less than about 4%.