Patents
US 4,426,516 A#4072402 Most CitedExpiredUnited States (USPTO)Utility

Polyester fiber dyeable under normal pressure

20Forward Citations (#4072402 Global)
0.5/yrCitation Velocity (#17332088 Global)
9.26Citation PageRank (#1204660 Global)
12Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A fiber consisting essentially of polyethylene terephthalate capable of being dyed under normal pressure and having an initial modulus at 30° C. of about 55 g/d to about 130 g/d, a relationship between a peak temperature ]T max (°C.)] at the peak of a dynamic mechanical loss tangent (tan δ) measured with a frequency of 110 Hz and a peak value of the dynamic mechanical loss tangent [(tan δ) max ] represented by the formula: (tan δ).sub.max ≦1×10.sup.-2 (T.sub.max -105) and a (tan δ) max of about 0.14 to about 0.30 and a dynamic mechanical loss tangent at 220° C. (tan δ 220 ) of at most about 0.055. The fiber is produced by subjecting a polyethylene terephthalate fiber obtained at a spinning speed of at least about 4000 m/min. to heat treatment at a temperature ranging from a temperature at which a dynamic modulus (E') of the fiber deviates from a tangent line at 180° C. of a logarithm of the E' of the fiber-temperature curve (T min ) plus 10° C. to a temperature of completion of melting (T m .sbsb.3) at a melting curve of the fiber measured by a differential scanning calorimeter (DSC) plus 10° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 20.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A fiber consisting essentially of polyethylene terephthalate capable of being dyed under normal pressure and having an initial modulus at 30° C. of about 55 g/d to about 130 g/d, a relationship between a peak temperature [T max (°C.)] at the peak of a dynamic mechanical loss tangent (tan δ) measured with a frequency of 110 Hz and a peak value of the dynamic mechanical loss tangent [(tan δ) max ] represented by the formula: (tan δ).sub.max ≧1×10.sup.-2 (T.sub.max -105) and a (tan δ) max of about 0.14 to about 0.30 and a dynamic mechanical loss tangent at 220° C. (tan δ 220 ) of at most

  2. Claim 2Depends on #1

    A fiber according to claim 1 not undergoing false twisting and having a T max (°C.) of at most about 105° C. and a (tan δ) max of at 1east about O.14.

  3. Claim 3Depends on #2

    A fiber according to claim 2 having a mean biref