Cobalt-base alloy having high strength and high toughness, production process of the same, and gas turbine nozzle
Abstract
A cobalt-base alloy comprises 0.2-1 wt % C 0.4-2 wt % Si, 0.2-1.5 wt % Mn, 5-15 wt % Ni, 20-35 wt % Cr, 3-15 wt % W, 0.003-0.1 wt % Ni, 20-35 wt % Cr, 3-15 wt % W, 0.003-0.1 wt % B, 0.05-1 wt % Nb, 0.01-1 wt % Ta, 2 wt % or less Fe, 30 ppm or less oxygen, 100 ppm or less nitrogen, and the balance of 45 wt % or more Co, wherein the content of Si is larger than that of Mn. The alloy is in a form of casting and has a structure containing a eutectic carbide and a secondary carbide dispersed therein. The cast alloy is produced through solution treatment at 1,100 DEG -1.200 DEG C., and aging treatment at 950 DEG -1,050 DEG C., and cooling rate after the solution treatment and after the aging treatment is 150 DEG to 300 DEG C./h. A gas turbine nozzle is made of a casting of the above-mentioned alloy.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 38.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A cobalt-base alloy having a high strength and a high toughness in the form of a casting, said alloy consisting essentially of 0.2 to 1% by weight of carboxy 0.4 to 2% by weight of silicon, 0.2 to 1.5% by weight of manganese, 5 to 15% by weight of nickel, 20 to 35% by weight of chromium, 3 to 15% by weight of tungsten, 0.003 to 0.1% by weight of boron, 0.05 to 1% by weight of niobium, 0.01 to 1% by weight of titanium, 2% by weight or lower of iron, 30 ppm or lower of oxygen and 100 ppm or lower of nitrogen with the balance being 45% by weight or higher of cobalt, wherein the content of the sil
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 38 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,080,202 A | Cobalt base alloy | 1978 | 5 |
| US 4,437,913 A | Cobalt base alloy | 1984 | 38 |