Patents
US 7,874,473 B2#16070125 Most CitedActiveUnited States (USPTO)Utility

Method for the soldering repair of a component in a vacuum and an adjusted partial oxygen pressure

7Forward Citations (#16070125 Global)
0.5/yrCitation Velocity (#17656301 Global)
1.36Citation PageRank (#26678292 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for the repair of a component by a solder is disclosed. The method is performed under specifically selected vacuum conditions in order to prevent oxidation and vaporization.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for a soldering repair of a component, comprising the steps of: repairing the component by soldering the component with a solder in a processing chamber, wherein the soldering includes: adjusting an oxygen partial pressure of less than 3.5*10 −6 mbar and greater than 10 −7 mbar in the processing chamber; and adjusting a total process pressure of less than 10 mbar and greater than 0.035 mbar in the processing chamber.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein prior to a heating of the component in the processing chamber with the solder a flushing of the processing chamber with an inert gas is performed.

  3. Claim 3Depends on #2

    The method according to claim 2 , wherein a throughput during the flushing lies between 0.21/min and 1 l/min.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
JP S59141395 ABrazing filler material—7
US 4,505,418 AMethod of direct bonding copper foils to oxide-ceramic substrates198549
US 4,514,751 ACompressively stresses titanium metallurgy for contacting passivated semiconductor devices198549
US 4,542,493 APickup stylus having fused diamond and ceramic bodies with conductive surfaces for capacitance disk records19853
US 4,789,412 ACobalt-base alloy having high strength and high toughness, production process of the same, and gas turbine nozzle198838
US 4,821,947 AFluxless application of a metal-comprising coating198925
US 4,908,185 ANichrome resistive element and method of making same19907
US 4,910,098 AHigh temperature metal alloy mixtures for filling holes and repairing damages in superalloy bodies199044
US 4,913,752 ANickel-based solder for high-temperature soldered joints199025
US 4,915,903 AProcess for forming composites having an intermetallic containing matrix1990103
US 4,925,829 AMethod for preparing thin film of compound oxide superconductor by ion beam techniques199024
JP H03128172 AMethod for joining member for vacuum equipment—8
US 5,096,110 AControl system for vacuum brazing process199217
US 5,121,875 AWave soldering in a protective atmosphere enclosure over a solder pot199237
EP 0,549,398 A1Process for welding or brazing strongly oxidisable metals—9
EP 0,486,489 B1High-temperature-resistant, corrosion-resistant coating, in particular for components of gas turbines1994471
US 5,364,011 AMicro soldering system for electronic components199482
US 5,529,805 AMethod for manufacturing a diamond article199652
US 5,565,401 ACatalyst comprising an assembly of at least one wire and its use in combustion or in post-combustion19963
EP 0,412,397 B1Rhenium-containing protective coating with high corrosion and oxidation resistance1998438
US 5,766,404 AMethods and apparatus for plasma treatment of workpieces199810
US 5,836,505 AJoining by brazing of ceramic materials containing silicon carbide199827
EP 0,786,017 B1Protective layer for protecting parts against corrosion, oxidation and excessive thermal stresses, as well as process for producing the same1999462