Patents
US 7,520,947 B2#9189982 Most CitedExpiredUnited States (USPTO)Utility

Cobalt alloys, methods of making cobalt alloys, and implants and articles of manufacture made therefrom

11Forward Citations (#9189982 Global)
0.7/yrCitation Velocity (#12208830 Global)
2.45Citation PageRank (#10472444 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Embodiments of the present invention provide methods of processing cobalt alloys including, in weight percent, from 26 to 30 chromium, from 5 to 7 molybdenum, and greater than 50 cobalt, the methods comprises cold working and aging the alloys such that after aging the cobalt alloys have a hardness of at least Rockwell C 50. Other embodiments provide methods of selectively cold working at least one portion of a cobalt alloy, and subsequently aging the alloy, such after aging, the selectively cold worked portions of the alloy have a higher hardness value then portions of the alloy that were not selectively cold worked. The present invention also discloses cobalt alloys, implants, and articles of manufacture made from cobalt alloys within the present invention.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 11.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of processing a cobalt alloy comprising from 26 to 30 weight percent chromium, from 5 to 7 weight percent molybdenum, up to 1.0 nickel, up to 0.75 iron, up to 1.0 manganese, and greater than 50 weight percent cobalt, the method comprising: cold working the cobalt alloy to achieve a total reduction of 5 to 25 percent; and aging the cold worked cobalt alloy at a temperature ranging from 900° F. to 1300° F. for a time period ranging from 1 hour to 24 hours; wherein after aging the cold worked cobalt alloy, the cobalt alloy has a hardness of at least Rockwell C 50, an elongation of at lea

  2. Claim 2Depends on #1

    The method of claim 1 wherein after cold working the cobalt alloy, at least a portion of the cobalt alloy comprises an fcc phase matrix with one or more regions of an hcp p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "ASTM 1537-00: Standard Specification for Wrought Cobalt-28Chromium-6Molybdenum Alloys for Surgical Implants (UNS R31537, UNS R31538, and UNS R31539)," ASTM International, Jan. 9, 2001, pp. 1-3.
  • "ASTM Designation E18-02: Standard Test Methods for Rockwell Hardness and Rockwell Superficial Hardness of Metallic Materials" ASTM International, (2003), pp. 1-15.
  • "ASTM Designation E384-99: Standard Test Method for Microindentation Hardness of Materials", ASTM International, (2003), pp. 1-24.
  • "ASTM Designation: E8-01: Standard Test Methods for Tension Testing of Metallic Materials" ASTM International, pp. 1-22.
  • "Chapter 5, The Physical and Mechanical Properties of Cobalt," Cobalt Monograph, Battelle Memorial Institute, (1960), pp. 73-81.