Nickel-based welding alloy also contains (preferred wt%): chromium 7.5 - 11; cobalt 8.0 -11.4; tungsten 2.8 - 6.9; melting point lowering agent 3 - 19.4; and at least one component chosen from scandium, zirconium, aluminum, titanium and tantalum. An independent claim is included for a method for repairing components (1) using the alloy (10) which is carried out at a uniform temperature or using a temperature gradient.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 1.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (15)

PatentTitleYearCitations
US 4,789,412 ACobalt-base alloy having high strength and high toughness, production process of the same, and gas turbine nozzle198838
US 4,908,185 ANichrome resistive element and method of making same19907
US 4,913,752 ANickel-based solder for high-temperature soldered joints199025
US 4,915,903 AProcess for forming composites having an intermetallic containing matrix1990103
EP 0,486,489 B1High-temperature-resistant, corrosion-resistant coating, in particular for components of gas turbines1994471
EP 0,412,397 B1Rhenium-containing protective coating with high corrosion and oxidation resistance1998438
EP 0,892,090 A1Method for manufacturing single crystal structures—479
EP 0,786,017 B1Protective layer for protecting parts against corrosion, oxidation and excessive thermal stresses, as well as process for producing the same1999462
US 5,993,980 AProtective coating for protecting a component from corrosion, oxidation and excessive thermal stress, process for producing the coating and gas turbine component1999116
WO 9,967,435 A1Directionally solidified casting with improved transverse stress rupture strength—516
US 6,024,792 AMethod for producing monocrystalline structures2000687
WO 0,044,949 A1Nickel base superalloy with good machinability—510
EP 1,306,454 A1Rhenium containing protective coating protecting a product against corrosion and oxidation at high temperatures—513
EP 1,319,729 A1High temperature resistant part, made of single-crystal or polycrystalline nickel-base superalloy—523
EP 1,204,776 B1High-temperature part and method for producing the same2004489