A modified propylene homopolymer (I) and/or modified propylene copolymer (II) having improved processability is prepared from a propylene homopolymer (III) having a melt index of 0.05 - 35 g/10 min at 230 degrees C and 2.16 kp and/or a copolymer (IV) containing 85-99.9 wt.%…
Panzer Ulf
Molded polyolefin articles of improved dimensional stability at elevated temperatures and improved stiffness and consist of mixtures of modified propylene polymers, which are synthesized by free radical coupling reactions or polymer-like reactions of functionalized polypropenes,…
Blow-moulded or injection-moulded polyolefin mouldings with improved heat distortion temperature and stiffness comprise: (a) 60-99.9, preferably 75-98 wt.% unmodified polypropylene polymer (I) and (b) 40-0.1, preferably 25-2 wt.% modified propylene polymer (B). (I) consists of…
Structurally isomeric poly(alkylethylenes) (SI-PAE) with improved processability and reduced melt instability, containing H and Y structures and with a psi index of 2-8 x 10<-3> kJ/mol/deg; psi = Tm . DELTA Hm . beta . s . Tg<-1>, where Tm = m.pt. (K), DELTA Hm =…
Polyolefin fibers and polyolefin yarns of high strength and elongation and textile fabrics produced therefrom. Polyolefin fibers and polyolefin yarns of high strength and elongation and textile fabrics produced therefrom, which consist of modified propylene polymers, unmodified…
A process (A) for the impregnation of filaments or filament bundles (rovings) with molten thermoplastic or liq. reaction resin (I), for the prodn. of fibre-reinforced material, comprises passing the fibres or rovings through an impregnation zone in the form of a damped wave.…
Polyolefin sheets and/or polyolefin coatings of substrates, such as textile fabrics, plastic sheets, paper, cardboard and metal with a high dimensional accuracy and thermal shock stability, consisting of modified polypropylene polymers or mixtures of modified polypropylene…
Polypropylene mixtures of increased stress-crack resistance and melt strength can be produced by irradiating polypropylene powders with low average particle diameters by low energy electron-beam accelerators with energies of 150 to 300 keV. The polypropylene mixtures produced…
Composites with a textile character with a high water vapor permeability and a high waterproofness, consisting of textile fabrics, film coatings and/or extrusion coatings of modified polypropylenes and unmodified polypropylenes and optionally of an intermediate layer of bonding…
Polyolefin foam materials of high dimensional stability at elevated temperatures are produced from modified polypropylenes and unmodified polypropylenes. The modified polypropylenes used are produced by mixing polypropylene particles with thermally decomposing free…
Fine-celled polyolefin foams of high dimensional stability at elevated temperatures and high stiffness, with foam densities ranging from 10 to 600 kg/m 3 , consisting of mixtures of polypropylenes and polyolefins, which were reacted with bifunctional, unsaturated monomers and/or…
Modified polypropylenes of improved processability are produced by a continuous method by absorptively charging polypropylene particles at 20° to 120° C. with a gas mixture, which contains oxygen and bifunctional, unsaturated monomers, and melting the mixture. The modified…
Polyolefin foam with a high heat distortion pt. and a density of 5-700 (preferably 10-500) kg/m<3>, consisting of 1-100 (preferably 5-100) wt% modified polypropylene (m-PP) and 0-99 (preferably (0-95) wt% unmodified PP (u-PP), in which the m-PP is obtained by (a) mixing PP…
Polyolefin fibers and polyolefin yarns of high strength and elongation and textile fabrics produced therefrom, which consist of modified propylene polymers, unmodified propylene polymers and adjuvants, are produced by melting the polyolefin mixtures in the extruder, transferring…
Continuous solid phase modification of polyolefins involves reacting polyolefin particles (I) with unsaturated monomers (II) in the presence of free radical initiators (III) undergoing thermal decomposition and optionally microwave-active additives. (I) consist of: (i) normal…
Continuous solid phase modification of polyolefins involves reacting polyolefin particles (I) with unsaturated monomers (II) in the presence of free radical initiators (III) undergoing thermal decomposition and optionally microwave-active additives. (I) consist of: (i) normal…
Modified polypropylenes of improved processability are produced by a continuous method by absorptively charging polypropylene particles at 20° to 120° C. with a gas mixture, which contains oxygen and bifunctional, unsaturated monomers, and melting the mixture. The modified…
Continuous modification of solid particles of linear or branched ethylene homo- or co-polymers, cycloolefin/ethylene copolymers, propylene homopolymers, statistical and/or block propylene copolymers, elastomeric polypropylenes, isotactic polybutene-1 and/or 4-Me-pentene-1 homo-…
A modified propylene homopolymer (I) and/or modified propylene copolymer (II) having improved processability is prepared from a propylene homopolymer (III) having a melt index of 0.05 - 35 g/10 min at 230 deg C and 2.16 kp and/or a copolymer (IV) containing 85-99.9 wt.%…
The invention relates to an acoustic component ( 1 ) of composite foam and a method of producing an acoustic component ( 1 ) comprising particles ( 2 ) or bars ( 11 ) of plastic foam, which are bound to one another by a binding agent ( 5 ). The particles ( 2 ) or bars ( 11 )…
A continuous process for the preparation of polypropylene mixtures with improved stress fracture resistance and melt strength comprises: (1) polypropylene powder with a mean particle size of 0.01-0.5 mm is intensively mixed under inert conditions at 20-150 deg.C whilst being…
Structurally isomeric poly(alkyl ethylenes) with H and Y structures, polymeric bridging segments and a Y index of 2×10 −3 to 8×10 −3 (kJ/mole/degree), have decreased instability in the melt and more advantageous processing properties. The structurally isomeric poly(alkyl…
The claims cover polyolefin fibres and yarns with high strength and elongation at break produced by melt processing, especially fibres with capillary titres of 1-10 dtex, elongation at break > 130% and tensile strength NOTLESS 15 cN/tex that are not redrawn, and textile…
Textile laminate with a water vapor permeability of more than 1000 (preferably more than 1800) g/m <2> per 24 hours and a water tightness corresponding to a water column of more than 500 mm (preferably more than 750) mm comprises: (A) a sheet of woven, knitted or nonwoven…
Polyolefin fibers and polyolefin yarns of high strength and elongation and textile fabrics produced therefrom, which consist of modified propylene polymers, unmodified propylene polymers and adjuvants, are produced by melting the polyolefin mixtures in the extruder, transferring…