Continuous process for preparing polypropylene compositions with improved stress crack resistance and high melt strength

8Forward Citations (#12886094 Global)
0.3/yrCitation Velocity (#27099044 Global)
2.23Citation PageRank (#12237130 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

A continuous process for the preparation of polypropylene mixtures with improved stress fracture resistance and melt strength comprises: (1) polypropylene powder with a mean particle size of 0.01-0.5 mm is intensively mixed under inert conditions at 20-150 deg.C whilst being exposed to a low intensity radiation dose of 0.05-12 (0.5-12) Mrad generated by a low energy electron accelerator operating at 150-300 keV; and (2) the addition of 0.05-2.5 mass % stabiliser, 0.1-1 mass % anti-static agent, 0.1-3 mass % pigment, optionally 0.05-5 mass % bifunctional unsaturated monomer, 0.05-1 mass % nucleating agent, 5-40 mass % filler and/or reinforcing agent, 2-20 mass % flame retardant and/or 0.01-1 mass % processing aid, before and/or after irradiation.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 8.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.