Abstract
Polypropylene mixtures of increased stress-crack resistance and melt strength can be produced by irradiating polypropylene powders with low average particle diameters by low energy electron-beam accelerators with energies of 150 to 300 keV. The polypropylene mixtures produced are suitable particularly for producing films, sheets, panels, coatings, pipes, hollow objects and foamed materials.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 48.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A continuous method for producing polypropylene mixtures of increased stress-crack resistance and melt strength comprising irradiating polypropylene powders with an average particle diameter of 0.01 to 0.5 mm under inert conditions using low-energy radiation from a low energy electron accelerator of 150 to 300 keV at a radiation dose of 0.05 to 12 Mrd and mixing the polypropylene powders for obtaining polypropylene mixtures of unmodified and modified polypropylene particles having increased stress-crack resistance and melt strength.
- Claim 2Depends on #1
The continuous method for producing polypropylene mixtures of increased stress-crack resistance and melt strength of claim 1, further comprising adding 2% by weight of volatile, bifunctional monomers.
- Claim 3Independent Claim
A method of forming films, sheets, fibers, panels, coatings, pipes, hollow bodies and f