The present invention provides a steel for nitriding purposes, which has a chemical composition comprising, in mass%, 0.10 to 0.20% of C, 0.01 to 0.7% of Si, 0.2 to 2.0% of Mn, 0.2 to 2.5% of Cr, not less than 0.01% and less than 0.19% of Al, more than 0.2% and not more than…
Tarui Toshimi
The present invention relates to a steel material giving more effective case hardening for improving the fatigue strength and is characterized by containing, by mass %, C: 0.01 to 0.3%, Si: less than 0.1%, Mn: 0.4 to 3%, Cr: 0.5 to 3%, and Al: 0.01 to 0.3%, further containing…
The disclosed steel contains, by mass: 0.10-0.55% carbon; 0.01-3% silicon; 0.1-2% manganese; and up to 1.5% vanadium and/or up to 3.0% molybdenum, with the vanadium content (V) and the molybdenum content (Mo) satisfying the relation V+½Mo > 0.4%. Said steel also contains one…
Disclosed is a wire material for a saw wire and a method for producing the same, wherein parameter P expressed by formula (1) for the C, Si, Mn, and Cr content is 1000 or higher. The metallographic structure includes an areal proportion of 98% or greater of drawn pearlite, and…
A saw wire includes a steel wire ( 11 ) having a steel strand ( 11 a ) with predetermined composition, an abrasive ( 13 ) fixed to the steel wire ( 11 ) by a fixing part ( 12 ), and an intermetallic compound ( 15 ) on an interface between the abrasive ( 13 ) and the fixing part…
A high strength steel material which is excellent in delayed fracture resistance containing, by mass %, C: 0.10 to 0.55%, Si: 0.01 to 3%, and Mn: 0.1 to 2%, further containing one or both of V: 1.5% or less and Mo: 3.0% or less, the contents of V and Mo satisfying…
Regarding contents of C, Si, Mn and Cr, a value of parameter P represented by the following (equation 1) is 1000 or more. A metallic structure contains wire-drawn pearlite in an area ratio of 98% or more, a diameter is 0.05 mm to 0.18 mm, a tensile strength is 4000 MPa or more,…
A steel which is excellent in delayed fracture resistance containing, by mass %, C: 0.10 to 0.55%, Si: 0.01 to 3%, and Mn: 0.1 to 2%, further containing one or more of Cr: 0.05 to 1.5%, V: 0.05 to 0.2%, Mo: 0.05 to 0.4%, Nb: 0.001 to 0.05%, Cu: 0.01 to 4%, Ni: 0.01 to 4%, and B:…
Provided is a steel for nitriding, which has a reduced strength before nitriding and therefore exhibits improved machinability. In the steel for nitriding, addionally, a nitrided layer with a large effective case depth can be formed for the purpose of improving the fatigue…
The present invention provides a steel wire, including chemical components of: C: 0.7-1.2 mass %; Si: 0.05-2.0 mass %; and Mn: 0.2-2.0 mass %, with a balance including Fe and inevitable impurities, in which the steel wire has a pearlite structure, the average C concentration at…
The present invention provides a steel for nitriding with a composition including, by mass %: C: 0.10% to 0.20%; Si: 0.01% to 0.7%; Mn: 0.2% to 2.0%; Cr: 0.2% to 2.5%; Al: 0.01% to less than 0.19%; V: over 0.2% to 1.0%; Mo: 0% to 0.54%; N: 0.001% to 0.01%; P limited to not more…
Provided is a steel wire containing, by mass, 0.7–1.2% carbon, 0.05–2.0% silicon, and 0.2–2.0% manganese, with the remainder comprising iron and unavoidable impurities. Said steel wire has a pearlite structure, a mean carbon concentration by mass of at most 0.2% in the central…
The present invention provides a high strength bolt excellent in delayed fracture resistance able to advantageously prevent hydrogen embrittlement as represented by the delayed fracture phenomenon occurring along with an increase in strength and causing a particular problem, and…
Disclosed is a high-strength Zn—Al coated steel wire for bridges with excellent corrosion resistance and fatigue properties, the Zn—Al coated steel wire includes: a steel wire; and a Zn—Al coating having a coating body layer and an Fe—Al alloy layer formed in an interface…
High strength machine parts excellent in fatigue strength which contain 0.1 to 1.2 mass % of C, and have a notch having a radius of curvature of 25 mm or less, wherein the surface thereof has an HV hardness of 250 or more and a surface layer of the notch has a compression…
Disclosed is a high-strength Zn-Al-plated steel wire for bridges, which comprises: a steel wire; a plated main body layer; and a Zn-Al-plated material comprising a Fe-Al alloy-produced layer that is generated on the interface between a surface layer of the steel wire and the…
The invention provides a steel material with satisfactory hydrogen embrittlement resistance, and particularly it relates to high-strength steel with satisfactory hydrogen embrittlement resistance and a strength of 1200 MPa or greater, as well as a process for production thereof.…
The disclosed steel contains, by mass, 0.10-0.55% carbon, 0.01-3% silicon, and 0.1-2% manganese. Said steel also contains one or more of the following: 0.05-1.5% chromium; 0.05-0.2% vanadium; 0.05-0.40% molybdenum; 0.001-0.05% niobium; 0.01-4% copper; 0.01-4% nickel; and…
Steel and steel shaped articles with an excellent delayed fracture resistance and a tensile strength of the 1600 MPa class or more, containing, by mass %, C: 0.20 to 0.60%, Si: 0.50% or less, Mn: over 0.10% to 3%, Al: 0.005 to 0.1%, Mo: over 3.0% to 10%, and, as needed, one or…
The present invention lowers the strength before nitriding to improve the machinability, while deepens the effective hardened case of the nitrided case for improving the fatigue strength. It provides steel for nitriding use containing, by mass %, C: 0.05 to 0.30%, Si: 0.003 to…
Disclosed is a saw wire which comprises: a steel wire (11) comprising a base steel wire (11a) having a given composition; abrasive grains (13) adhered to the steel wire (11) by means of an adhesion part (12); and an intermetallic compound (15) formed at the interface between the…
The present invention provides a steel for nitriding with a composition including, by mass %: C: 0.10% to 0.20%; Si: 0.01% to 0.7%; Mn: 0.2% to 2.0%; Cr: 0.2% to 2.5%; Al: 0.01% to less than 0.19%; V: over 0.2% to 1.0%; Mo: 0% to 0.54%; N: 0.001% to 0.01%; P limited to not more…
A steel which is excellent in delayed fracture resistance containing, by mass %, C: 0.10 to 0.55%, Si: 0.01 to 3%, and Mn: 0.1 to 2%, further containing one or more of Cr: 0.05 to 1.5%, V: 0.05 to 0.2%, Mo: 0.05 to 0.4%, Nb: 0.001 to 0.05%, Cu: 0.01 to 4%, Ni: 0.01 to 4%, and B:…
A high strength steel product excellent in characteristics of the resistance to hydrogen embrittlement, which has a specific chemical composition, and contains, as trapping sites for trapping hydrogen with a specific trapping energy, at least one of single and composite…
A saw wire includes a steel wire ( 11 ) having a steel strand ( 11 a ) with predetermined composition, an abrasive ( 13 ) fixed to the steel wire ( 11 ) by a fixing part ( 12 ), and an intermetallic compound ( 15 ) on an interface between the abrasive ( 13 ) and the fixing part…