The present invention provides a steel for nitriding purposes, which has a chemical composition comprising, in mass%, 0.10 to 0.20% of C, 0.01 to 0.7% of Si, 0.2 to 2.0% of Mn, 0.2 to 2.5% of Cr, not less than 0.01% and less than 0.19% of Al, more than 0.2% and not more than…
Hirakami Daisuke
The present invention relates to a steel material giving more effective case hardening for improving the fatigue strength and is characterized by containing, by mass %, C: 0.01 to 0.3%, Si: less than 0.1%, Mn: 0.4 to 3%, Cr: 0.5 to 3%, and Al: 0.01 to 0.3%, further containing…
The disclosed steel contains, by mass: 0.10-0.55% carbon; 0.01-3% silicon; 0.1-2% manganese; and up to 1.5% vanadium and/or up to 3.0% molybdenum, with the vanadium content (V) and the molybdenum content (Mo) satisfying the relation V+½Mo > 0.4%. Said steel also contains one…
A process for producing a steel material is provided which includes subjecting a highly strengthened steel material (W) to a heat treatment to thereby cause part of the steel material to have a lower hardness than the remainder of the steel material (W). The heat treatment…
A high strength steel material which is excellent in delayed fracture resistance containing, by mass %, C: 0.10 to 0.55%, Si: 0.01 to 3%, and Mn: 0.1 to 2%, further containing one or both of V: 1.5% or less and Mo: 3.0% or less, the contents of V and Mo satisfying…
A steel which is excellent in delayed fracture resistance containing, by mass %, C: 0.10 to 0.55%, Si: 0.01 to 3%, and Mn: 0.1 to 2%, further containing one or more of Cr: 0.05 to 1.5%, V: 0.05 to 0.2%, Mo: 0.05 to 0.4%, Nb: 0.001 to 0.05%, Cu: 0.01 to 4%, Ni: 0.01 to 4%, and B:…
Provided is a steel for nitriding, which has a reduced strength before nitriding and therefore exhibits improved machinability. In the steel for nitriding, addionally, a nitrided layer with a large effective case depth can be formed for the purpose of improving the fatigue…
The present invention provides a steel for nitriding with a composition including, by mass %: C: 0.10% to 0.20%; Si: 0.01% to 0.7%; Mn: 0.2% to 2.0%; Cr: 0.2% to 2.5%; Al: 0.01% to less than 0.19%; V: over 0.2% to 1.0%; Mo: 0% to 0.54%; N: 0.001% to 0.01%; P limited to not more…
The present invention provides a wire rod with a composition at least including: C: 0.95-1.30 mass %; Si: 0.1-1.5 mass %; Mn: 0.1-1.0 mass %; Al: 0-0.1 mass %; Ti: 0-0.1 mass %; P: 0-0.02 mass %; S: 0-0.02 mass %; N: 10-50 ppm; O: 10-40 ppm; and a balance including Fe and…
The invention provides a steel material with satisfactory hydrogen embrittlement resistance, and particularly it relates to high-strength steel with satisfactory hydrogen embrittlement resistance and a strength of 1200 MPa or greater, as well as a process for production thereof.…
The disclosed steel contains, by mass, 0.10-0.55% carbon, 0.01-3% silicon, and 0.1-2% manganese. Said steel also contains one or more of the following: 0.05-1.5% chromium; 0.05-0.2% vanadium; 0.05-0.40% molybdenum; 0.001-0.05% niobium; 0.01-4% copper; 0.01-4% nickel; and…
The present invention lowers the strength before nitriding to improve the machinability, while deepens the effective hardened case of the nitrided case for improving the fatigue strength. It provides steel for nitriding use containing, by mass %, C: 0.05 to 0.30%, Si: 0.003 to…
A wire material comprising 0.95 to 1.30 mass% of C, 0.1 to 1.5 mass% of Si, 0.1 to 1.0 mass% of Mn, 0 to 0.1 mass% of Al, 0 to 0.1 mass% of Ti, 0 to 0.02 mass% of P, 0 to 0.02 mass% of S, 10 to 50 ppm of N, 10 to 40 ppm of O, and the remainder containing at least Fe and…
The present invention provides a steel for nitriding with a composition including, by mass %: C: 0.10% to 0.20%; Si: 0.01% to 0.7%; Mn: 0.2% to 2.0%; Cr: 0.2% to 2.5%; Al: 0.01% to less than 0.19%; V: over 0.2% to 1.0%; Mo: 0% to 0.54%; N: 0.001% to 0.01%; P limited to not more…
A steel which is excellent in delayed fracture resistance containing, by mass %, C: 0.10 to 0.55%, Si: 0.01 to 3%, and Mn: 0.1 to 2%, further containing one or more of Cr: 0.05 to 1.5%, V: 0.05 to 0.2%, Mo: 0.05 to 0.4%, Nb: 0.001 to 0.05%, Cu: 0.01 to 4%, Ni: 0.01 to 4%, and B:…
A high strength steel product excellent in characteristics of the resistance to hydrogen embrittlement, which has a specific chemical composition, and contains, as trapping sites for trapping hydrogen with a specific trapping energy, at least one of single and composite…
The present invention provides a wire rod with a composition at least including: C: 0.95-1.30 mass %; Si: 0.1-1.5 mass %; Mn: 0.1-1.0 mass %; Al: 0-0.1 mass %; Ti: 0-0.1 mass %; P: 0-0.02 mass %; S: 0-0.02 mass %; N: 10-50 ppm; O: 10-40 ppm; and a balance including Fe and…
The invention provides a steel material with satisfactory hydrogen embrittlement resistance, and particularly it relates to high-strength steel with satisfactory hydrogen embrittlement resistance and a strength of 1200 MPa or greater, as well as a process for production thereof.…