Patents
Assignee / Organization

Chida Tetsushi

150Total Forward Citations
13Indexed Patents
12Avg Citations / Patent
9Portfolio H-Index
WO 2012/067181 A1#3031509 Most Cited · 25 citations1.8/yr · PR 3.95PendingWO · Application
Steel for nitriding purposes, and nitrided member

The present invention provides a steel for nitriding purposes, which has a chemical composition comprising, in mass%, 0.10 to 0.20% of C, 0.01 to 0.7% of Si, 0.2 to 2.0% of Mn, 0.2 to 2.5% of Cr, not less than 0.01% and less than 0.19% of Al, more than 0.2% and not more than…

US 2011186182 A1#4150417 Most Cited · 20 citations1.3/yr · PR 4.38PendingUS · Application
Steel for nitrocarburizing and nitrocarburized parts

The present invention relates to a steel material giving more effective case hardening for improving the fatigue strength and is characterized by containing, by mass %, C: 0.01 to 0.3%, Si: less than 0.1%, Mn: 0.4 to 3%, Cr: 0.5 to 3%, and Al: 0.01 to 0.3%, further containing…

WO 2011/111872 A1#4559913 Most Cited · 19 citations1.3/yr · PR 3.18PendingWO · Application
High-strength steel and high-strength bolt with excellent resistance to delayed fracture, and manufacturing method therefor

The disclosed steel contains, by mass: 0.10-0.55% carbon; 0.01-3% silicon; 0.1-2% manganese; and up to 1.5% vanadium and/or up to 3.0% molybdenum, with the vanadium content (V) and the molybdenum content (Mo) satisfying the relation V+½Mo > 0.4%. Said steel also contains one…

US 2012247618 A1#6636268 Most Cited · 14 citations1.0/yr · PR 4.15PendingUS · Application
High strength steel material and high strength bolt excellent in delayed fracture resistance and methods of production of same

A high strength steel material which is excellent in delayed fracture resistance containing, by mass %, C: 0.10 to 0.55%, Si: 0.01 to 3%, and Mn: 0.1 to 2%, further containing one or both of V: 1.5% or less and Mo: 3.0% or less, the contents of V and Mo satisfying…

US 2012298262 A1#7760690 Most Cited · 13 citations0.9/yr · PR 2.05PendingUS · Application
High strength steel and high strength bolt excellent in delayed fracture resistance and methods of production of same

A steel which is excellent in delayed fracture resistance containing, by mass %, C: 0.10 to 0.55%, Si: 0.01 to 3%, and Mn: 0.1 to 2%, further containing one or more of Cr: 0.05 to 1.5%, V: 0.05 to 0.2%, Mo: 0.05 to 0.4%, Nb: 0.001 to 0.05%, Cu: 0.01 to 4%, Ni: 0.01 to 4%, and B:…

WO 2010/147224 A1#7524309 Most Cited · 13 citations0.8/yr · PR 2.66PendingWO · Application
Steel for nitriding and nitrided steel components

Provided is a steel for nitriding, which has a reduced strength before nitriding and therefore exhibits improved machinability. In the steel for nitriding, addionally, a nitrided layer with a large effective case depth can be formed for the purpose of improving the fatigue…

US 2012291927 A1#10418922 Most Cited · 10 citations0.7/yr · PR 2.12PendingUS · Application
Drawn heat treated steel wire for high strength spring use and pre-drawn steel wire for high strength spring use

Drawn heat treated steel wire for high strength spring use is provided containing, by mass %, C: 0.67% to less than 0.9%, Si: 2.0 to 3.5%, Mn: 0.5 to 1.2%, Cr: 1.3 to 2.5%, N: 0.003 to 0.007%, and Al: 0.0005% to 0.003%, having Si and Cr satisfying the following formula:…

US 2013087250 A1#10745125 Most Cited · 10 citations0.8/yr · PR 1.73PendingUS · Application
Steel for nitriding and nitrided part

The present invention provides a steel for nitriding with a composition including, by mass %: C: 0.10% to 0.20%; Si: 0.01% to 0.7%; Mn: 0.2% to 2.0%; Cr: 0.2% to 2.5%; Al: 0.01% to less than 0.19%; V: over 0.2% to 1.0%; Mo: 0% to 0.54%; N: 0.001% to 0.01%; P limited to not more…

WO 2012/005373 A1#11846454 Most Cited · 9 citations0.6/yr · PR 1.91PendingWO · Application
Drawn and heat-treated steel wire for high-strength spring, and undrawn steel wire for high-strength spring

A drawn and heat-treated steel wire for a high-strength spring, which comprises, in mass%, not less than 0.67% and less than 0.9% of C, 2.0-3.5% of Si, 0.5-1.2% of Mn, 1.3-2.5% of Cr, 0.003-0.007% of N, 0.0005-0.003% of Al, Si and Cr in such amounts that the following formula:…

WO 2011/111873 A1#14628159 Most Cited · 7 citations0.5/yr · PR 2.16PendingWO · Application
High-strength steel and high-strength bolt with excellent resistance to delayed fracture, and manufacturing method therefor

The disclosed steel contains, by mass, 0.10-0.55% carbon, 0.01-3% silicon, and 0.1-2% manganese. Said steel also contains one or more of the following: 0.05-1.5% chromium; 0.05-0.2% vanadium; 0.05-0.40% molybdenum; 0.001-0.05% niobium; 0.01-4% copper; 0.01-4% nickel; and…

US 2012080122 A1#26229358 Most Cited · 4 citations0.3/yr · PR 1.22PendingUS · Application
Steel for nitriding use and nitrided part

The present invention lowers the strength before nitriding to improve the machinability, while deepens the effective hardened case of the nitrided case for improving the fatigue strength. It provides steel for nitriding use containing, by mass %, C: 0.05 to 0.30%, Si: 0.003 to…

US 8,876,988 B2#34059852 Most Cited · 3 citations0.2/yr · PR 0.96ActiveUS · Utility
Steel for nitriding and nitrided part
Inventors: Chida Tetsushi, Kubota Manabu, Tarui Toshimi, Hirakami Daisuke, Hashimura MasayukiAssignee: Chida Tetsushi, Kubota ManabuFiled 2011-11-17 · Granted 2014-11-04

The present invention provides a steel for nitriding with a composition including, by mass %: C: 0.10% to 0.20%; Si: 0.01% to 0.7%; Mn: 0.2% to 2.0%; Cr: 0.2% to 2.5%; Al: 0.01% to less than 0.19%; V: over 0.2% to 1.0%; Mo: 0% to 0.54%; N: 0.001% to 0.01%; P limited to not more…

US 8,951,365 B2#33988621 Most Cited · 3 citations0.3/yr · PR 0.97ActiveUS · Utility
High strength steel and high strength bolt excellent in delayed fracture resistance and methods of production of same
Inventors: Hirakami Daisuke, Chida Tetsushi, Tarui ToshimiAssignee: Hirakami Daisuke, Chida TetsushiFiled 2011-03-11 · Granted 2015-02-10

A steel which is excellent in delayed fracture resistance containing, by mass %, C: 0.10 to 0.55%, Si: 0.01 to 3%, and Mn: 0.1 to 2%, further containing one or more of Cr: 0.05 to 1.5%, V: 0.05 to 0.2%, Mo: 0.05 to 0.4%, Nb: 0.001 to 0.05%, Cu: 0.01 to 4%, Ni: 0.01 to 4%, and B:…