A high-strength stainless steel having excellent mechanical properties and corrosion resistance in high-pressure hydrogen gas environments is disclosed. A container for high-pressure hydrogen gas made of such a stainless steel is also disclosed. The stainless steel has a…
Semba Hiroyuki
An austenitic stainless steel for a hydrogen gas, which has a chemical composition, in mass %, that C: 0.10 % or less, Si: 1.0 % or less, Mn: 0.01 to 30 %, P: 0.040 % or less, S: 0.01 % or less, Cr: 15 to 30 %, Ni: 5.0 to 30 %, Al: 0.10 % or less, N: 0.001 to 0.30 % and the…
An austenitic stainless steel for high-pressure hydrogen gas, characterized by containing, in terms of mass%, up to 0.10% C, up to 1.0% Si, 3-7%, excluding 7%, Mn, 15-30% Cr, 10-17%, excluding 17%, Ni, up to 0.10% Al, 0.10-0.50% N, and 0.01-1.0% V and/or 0.01-0.50% Nb, with the…
Disclosed is a steel which does not suffer from hydrogen embrittlement even when the steel is used in a hydrogen gas environment. Also disclosed are a method for producing such a steel and a container for high-pressure hydrogen gas or other hardware made of such a steel. A steel…
Provided is a coaxial cable connecting structure having both mechanical reliability relating to bendability and electrical characteristics relating to impedance matching and EMI characteristics. A coaxial cable harness to be used for such coaxial cable connecting structure and a…
A stainless steel for a high pressure hydrogen gas, characterized in that it has a chemical composition, in mass %: C: 0.02 % or less, Si: 1.0 % or less, Mn: 3 to 30 %, Cr: more than 22 % and up to 30 %, Ni: 17 to 30 %, V: 0.001 to 1.0 %, N: 0.10 to 0.50 %, Al: 0.10 % or less,…
Disclosed is a Ni‑based heat-resistant alloy that contains C ≦ 0.1%, Si ≦ 1%, Mn≦1%, Cr: 15% to less than 28%, Fe ≦ 15%, W: more than 5‑20%, Al: more than 0.5‑2%, Ti: more than 0.5‑2%, Nd: 0.001-0.1%, B: 0.0005-0.01%, and the remainder comprising Ni and impurities, wherein the…
An austenitic stainless steel for use in a hydrogen gas atmosphere comprises, in mass %, C: 0.10% or less, Si: 1.0% or less, Mn: 0.01 to 30%, P: 0.040% or less, S: 0.01% or less, Cr: 15 to 30%, Ni: 5.0 to 30%, Al: 0.10% or less, N: 0.001 to 0.30 % with the balance Fe and…
An austenitic stainless steel, which comprises by mass %, C: 0.04 to 0.18%, Si≦1.5%, Mn≦2.0%, Ni: 6 to 30%, Cr: 15 to 30%, N: 0.03 to 0.35%, sol. Al≦0.03% and further contains one or more elements selected from Nb≦1.0%, V≦0.5% and Ti≦0.5%, with the balance being Fe and…
Disclosed is an austenitic stainless steel which comprises the following components: C: 0.04-0.18%, Si: 1.5% or less, Mn: 2.0% or less, Ni: 6-30%, Cr: 15-30%, N: 0.03-0.35%, and sol.Al: 0.03% or less, and which further comprises at least one component selected from 1.0% or less…
A heat-resistant austenitic alloy which contains 0.02-0.15%, excluding 0.02%, C, up to 2% Si, up to 3% Mn, up to 0.03% P, up to 0.01% S, 28-38% Cr, 40-60%, excluding 40%, Ni, up to 20% (including 0%) Co, 3-15%, excluding 3%, W, 0.05-1.0% Ti, 0.005-0.2% Zr, and 0.01-0.3% Al and…
There is provided an austenitic stainless steel for high-pressure hydrogen gas consisting, by mass percent, of C: 0.10% or less, Si: 1.0% or less, Mn: 3% or more to less than 7%, Cr: 15 to 30%, Ni: 10% or more to less than 17%, Al: 0.10% or less, N: 0.10 to 0.50%, and at least…
A steel which does not suffer from hydrogen embrittlement contains 0.3-30% of Cr as the base material, and has an oxide film having a thickness of 100 nm or more formed on its surface. The oxide film contains at least two elements selected among Fe, Cr and Al in the form of…
Disclosed is an austenitic heat-resistant alloy, which contains 0.15% or less of C, 2% or less of Si, 3% or less of Mn, 40-60% of Ni, 0.03-25% of Co, 15% or more but less than 28% of Cr, 12% or less of Mo and/or less than 4% of W with the total being 0.1-12%, 0.001-0.1% of Nd,…
A weld joint having a base material and a weld metal both of an austenitic steel, wherein the weld metal has a chemical composition, in mass %, that C: 0.04 % or less, Si: 1.0 % or less, Mn: 3 % or less, P: 0.02 % or less, S: 0.005 % or less, Cr: 15 to 25 %, Ni: 30 % or more,…
A weld joint having a base material and a weld metal both of an austenitic steel, wherein the weld metal has a chemical composition, in mass %, that C: 0.04% or less, Si: 1.0% or less, Mn: 3% or less, P: 0.02% or less, S: 0.005% or less, Cr: 15 to 25%, Ni: 30% or more, Mo: 10%…
Provided are a cable harness comprising an ultrathin coaxial cable which can satisfy the performance of a cable for a signal and a cable for a power source and which can be easily and accurately connected with a connecter terminal and the like of a terminal portion, the cable…
An Ni-based heat-resistant alloy which contains 0.15% or less of C, 2% or less of Si, 3% or less of Mn, 0.03% or less of P, 0.01% or less of S, 15% or more but less than 28% of Cr, 3-15% of Mo, more than 5% but 25% or less of Co, 0.2-2% of Al, 0.2-3% of Ti, from fn to 0.08% of…
In each of plural coaxial cables 11 , a tip portion of an outer sheath 12 is removed and portions of an outer conductor 13 , an insulator 14 , and a center conductor 15 are exposed in this order in a step-like manner. A ground bar 20 having lock nails 23 for locking the coaxial…
An austenitic heat resistant alloy consisting of, by mass percent, C: 0.15% or less, Si: 2% or less, Mn: 3% or less, Ni: 40 to 60%, Co: 0.03 to 25%, Cr: 15% or more and less than 28%, either one or both of Mo: 12% or less and W: less than 4%, the total content thereof being 0.1…
An austenitic heat resistant alloy, which contains, by mass percent, C≦0.15%, Si≦2%, Mn≦3%, Ni: 40 to 80%, Cr: 15 to 40%, W and Mo: 1 to 15% in total content, Ti≦3%, Al≦3%, N≦0.03%, O≦0.03%, with the balance being Fe and impurities, and among the impurities P≦0.04%, S≦0.03%,…
Disclosed is a welding material for an Ni-based heat-resistant alloy, which has a chemical composition that contains 0.06-0.18% of C, 0.5% or less of Si, 1.5% or less of Mn, 46-56% of Ni, 10-15% of Co, 20-25% of Cr, more than 10.0% but 14.0% or less of Mo, 0.01-0.5% of Ti,…
Provided is a low alloy steel for high-pressure hydrogen gas environments, which contains, by mass percent, C: 0.15 to 0.60%, Si: 0.05 to 0.5%, Mn: 0.05 to 3.0%, P: not more than 0.025%, S: not more than 0.010%, Al: 0.005 to 0.10%, Mo: 0.5 to 3.0%, V: 0.05 to 0.30%, O (oxygen):…
A Ni-based heat resistant alloy as pipe, plate, rod, forgings and the like consists of C≦0.15%, Si≦2%, Mn≦3%, P≦0.03%, S≦0.01%, Cr: 15% or more and less than 28%, Mo: 3 to 15%, Co: more than 5% and not more than 25%, Al: 0.2 to 2%, Ti: 0.2% to 3%, Nd: fn to 0.08%, and O≦0.4Nd,…
A high strength, ductile, and tough Ni-base heat resistant alloy comprises by mass percent, C: 0.1% or less, Si: 1% or less, Mn: 1% or less, Cr: not less than 15% to less than 28%, Fe: 15% or less, W: more than 5% to not more than 20%, Al: more than 0.5% to not more than 2%, Ti:…