Ni-base heat resistant alloy
Abstract
A high strength, ductile, and tough Ni-base heat resistant alloy comprises by mass percent, C: 0.1% or less, Si: 1% or less, Mn: 1% or less, Cr: not less than 15% to less than 28%, Fe: 15% or less, W: more than 5% to not more than 20%, Al: more than 0.5% to not more than 2%, Ti: more than 0.5% to not more than 2%, Nd: 0.001 to 0.1% and B: 0.0005 to 0.01%, with the balance being Ni and impurities. Impurity contents of P, S, Sn, Pb, Sb, Zn and As are P: 0.03% or less, S: 0.01% or less, Sn: 0.020% or less, Pb: 0.010% or less, Sb: 0.005% or less, Zn: 0.005% or less and As: 0.005% or less, and formulas of [0.015≦Nd+13.4×B≦0.13], [Sn+Pb≦0.025] and [Sb+Zn +As≦0.010] are met.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 3.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A Ni-base heat resistant alloy, which comprises by mass percent, C: 0.1% or less, Si: 1% or less, Mn: 1% or less, Cr: not less than 15% to less than 28%, Fe: 15% or less, W: more than 5% to not more than 20%, Al: more than 0.5% to not more than 1.65%, Ti: more than 0.5% to not more than 2%, Nd: 0.001 to 0.1% and B: 0.0005 to 0.01%, with the balance being Ni and impurities, in which the contents of P, S, Sn, Pb, Sb, Zn and As among the impurities are P: 0.03% or less, S: 0.01% or less, Sn: 0.020% or less, Pb: 0.010% or less, Sb: 0.005% or less, Zn: 0.005% or less and As: 0.005% or less, and fur
- Claim 2Independent Claim
The Ni-base he
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗