US 8,313,591 B2#16158135 Most CitedActiveUnited States (USPTO)Utility

Austenitic heat resistant alloy

7Forward Citations (#16158135 Global)
0.5/yrCitation Velocity (#15955869 Global)
1.26Citation PageRank (#29887583 Global)
28Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An austenitic heat resistant alloy, which contains, by mass percent, C≦0.15%, Si≦2%, Mn≦3%, Ni: 40 to 80%, Cr: 15 to 40%, W and Mo: 1 to 15% in total content, Ti≦3%, Al≦3%, N≦0.03%, O≦0.03%, with the balance being Fe and impurities, and among the impurities P≦0.04%, S≦0.03%, Sn≦0.1%, As≦0.01%, Zn≦0.01%, Pb≦0.01% and Sb≦0.01%, and satisfies the conditions [P1=S+{(P+Sn)/2}+{(As+Zn+Pb+Sb)/5}≦0.050], [0.2≦P2=Ti+2Al≦7.5−10×P1], [P2≦9.0−100×O] and [N≦0.002×P2+0.019] can prevent both the liquation crack in the HAZ and the brittle crack in the HAZ and also can prevent defects due to welding fabricability, which occur during welding fabrication, and moreover has excellent creep strength at high temperatures. Therefore, the alloy can be used suitably as a material for constructing high temperature machines and equipment, such as power generating boilers, plants for the chemical industry and so on. The ally may contain a specific amount or amounts of one or more elements selected from Co, B, Ta, Hf, Nb, Zr, Ca, Mg, Y, La, Ce and Nd.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An austenitic heat resistant alloy, which consists of, by mass percent, C: not more than 0.15%, Si: not more than 2%, Mn: not more than 3%, Ni: 40 to 80%, Cr: 15 to 40%, W: not less than 3%, and W and Mo: 3 to 15% in total content, Ti: not more than 3%, Al: not more than 3%, Co: 9.85 to 20%, N: not more than 0.03% and O: not more than 0.03%, with the balance being Fe and impurities, in which the contents of P, S, Sn, As, Zn, Pb and Sb among the impurities are P: not more than 0.04%, S: not more than 0.03%, Sn: not more than 0.1%, As: not more than 0.01%, Zn: not more than 0.01%, Pb: not more t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (28)

PatentTitleYearCitations
JP S5184727 ATainetsuseinoryokonagokin—19
JP S5423016 AMethod of producing austenitic stainless steel containing nickel—5
JP S5845359 AHeat and oxidation resistant chromium-iron alloy—2
JP S59182919 AProduction of high-tensile low-alloy steel pipe—4
JP S60100640 AHigh-chromium alloy having excellent resistance to heat and corrosion—13
JP S61179833 AHighly corrosion resistant austenitic stainless steel having superior strength at high temperature—13
JP S6455352 AHeat-resisting alloy—11
JP H02200756 AHigh strength heat resisting steel excellent in workability—11
US 5,021,215 AHigh-strength, heat-resistant steel with improved formability and method thereof199143
JP H07150277 ANickel-base alloy having excellent stress breaking strength and grain size controll-ability—21
JP H07216511 AHigh chromium austenitic heat resistant alloy excellent in strength at high temperature—35
JP H07331390 AHigh chromium austenitic heat resistant alloy—18
JP H08127848 AHigh chromium austenitic heat resistant alloy excellent in high temperature strength—30
US 5,543,109 AHeat resistant high chromium austenitic alloy excellent in strength at elevated temperatures199632
JP H08218140 AHigh chromium austenitic heat resistant alloy excellent in high temperature strength and high temperature corrosion resistance—18
JP H09157779 ALow thermal expansion nickel base superalloy and its production—54
US 5,716,468 AProcess for producing high-and low-pressure integral-type turbine rotor199819
JP 2002518599 A最新の超臨界ボイラーの管用合金—17
US 6,447,716 B1Welding electrode made of a nickel-based alloy and the corresponding alloy200220
US 2003005981 A1Ni-base heat resistant alloy and welded joint thereof—49
US 6,623,869 B1Metal material having good resistance to metal dusting2003121
US 2003198567 A1Austenitic stainless steel excellent in high temperature strength and corrosion resistance, heat resistant pressurized parts, and the manufacturing method thereof—12

Non-Patent Literature (5)

  • Davis, J.R. et al., "ASM Specialty Handbook, Nickel, Cobalt and Their Alloys", Dec. 1, 2000, XP002183407, Table 2.
  • R. Younger et al., "Heat-Affected Zone Cracking in Welded Austenitic Steels During Heat Treatment", British Welding Journal, Dec. 1961, p. 579-587.
  • R. Younger et al., "Heat-affected zone cracking in welded high-temperature austenitic steels", Journal of the Iron and Steel Institute, Oct. 1960, p. 188-193.
  • T. Naiki et al., "Cracking in Welded 18 Cr-12 Ni-Nb Steel during Stress Relieving", Ishikawajima Harima Engineering Review, vol. 15, No. 2, 1975, p. 209.
  • Welding and Joining Handbook, 2nd Edition, edited by the Japan Welding Society (2003, Maruzen), p. 948-953.