Provided is a cover glass for display devices, which comprises a high-strength and transparent crystallized glass. A crystallized glass for display devices, which has a transmittance (T 400nm ) of light having a wavelength of 400 nm of more than 10% when the glass is prepared…
Koike Akio
The present invention relates to an alkali free glass in which the strain point is 725°C or more, the average thermal expansion coefficient at 50-300°C is 3x10 -7 -40x10 -7 /°C, the temperature (T 2 ) at which glass viscosity becomes 10 2 dPa·s is 1710°C or less, and the…
It is to provide a silica glass containing TiO2, having a wide temperature range where wherein the coefficient of thermal expansion becomes is substantially zero. A silica glass containing TiO2, which has a TiO2 concentration of from 3 to 10 mass%, a OH group concentration of at…
The present invention relates to a chemically strengthened glass for a display device in which the visible light transmittance (Tva) obtained at a thickness of 1 mm using a light source (A) is 50% or higher and less than 91%, and the excitation purity (Pe) at a thickness of 1 mm…
In order to provide a walking assistance device capable of favorably providing an assisting force for maintaining the upright posture while reducing the sense of pressure when worn by the user, a hip support member ( 1 ) of the walking assisting device, which comprises an…
A silica glass containing TiO2, which has a fictive temperature of at most 1, 200 C, a F concentration of at least 100 ppm and a coefficient of thermal expansion of 0 ± 200 ppb/°c from 0 to 100°c. A process for producing a silica glass containing TiO2, which comprises a step of…
Disclosed is a glass substrate which is rarely detached from a silicon wafer when the glass substrate is laminated on and attached to the silicon wafer and the resulting laminate is subsequently heated, and which has a plurality of through-holes. Specifically disclosed is a…
A silica glass containing TiO2, which has a fictive temperature of at most 1,200 °C, an OH group concentration of at most 600 ppm and a coefficient of thermal expansion of 0± 200 ppb/ C from 0 to 100 °C.
Provided is a low-cost near-infrared cut-off filter glass that minimizes near-infrared transmittance while maintaining high UV transmittance. The UV-transmitting near-infrared cut-off filter glass contains, represented by mass%, 50 to 85% P 2 O 5 , 1 to 20% Al 2 O 3 , 1 to 5% B…
The present invention provides float glass for chemical strengthening which enables warping after chemical strengthening to be effectively minimized, and enables polishing etc. prior to chemical strengthening to be omitted or simplified. The present invention pertains to float…
A silica glass containing TiO2, characterized in that the fluctuation of the refractive index (Δn) is at most 2 ~10-4 within an area of 30 mm ~ 30 mm in at least one plane. A silica glass containing TiO2, characterized in that the TiO2 concentration is at least 1 mass%, and the…
Conventional TiO2-SiO2 glass contains hydrogen atoms substantially and during deposition under ultrahigh vacuum condition, the hydrogen molecules will diffuse in the chamber, and H2 molecules will be taken into a film thereby formed. Hydrogen molecules will readily diffuse and…
The present invention relates to a substrate for EUV lithography optical member, comprising a silica glass containing TiO 2 , in which the substrate has two opposite surfaces, and the substrate has temperatures at which a coefficient of linear thermal expansion (CTE) is 0 ppb/°C…
The present invention relates to a substrate for EUV lithography optical member, comprising a silica glass containing TiO 2 , in which the substrate has two opposite surfaces, and the substrate has temperatures at which a coefficient of linear thermal expansion (CTE) is 0 ppb/°…
A TiO 2 -containing glass (TiO 2 -SiO 2 glass) which exhibits a coefficient of thermal expansion of approximately zero at room temperature and makes it possible by virtue of the release of hydrogen from the glass to keep the physical properties of the multilayer of an exposure…
Disclosed is a method for producing a TiO 2 -SiO 2 glass body, which comprises a step in which a TiO 2 -SiO 2 glass body after transparent vitrification is maintained within a temperature range from T 1 -90 (°C) to T 1 -220 (°C) for 120 hours or more, with T 1 (°C) being the…
The present invention provides a TiO2-SiO2 glass having suitable thermal expansion properties as an optical member of an exposure tool for EUVL. The present invention relates to a TiO2-containing silica glass having a TiO2 content of from 3 to 9 % by mass; a temperature, at…
A silica glass containing from 3 to 10 mass% of TiO2, which has a coefficient of thermal expansion from 0 to 100 °C, i.e. CTE0 to 100, of 0 ± 300 ppb/ °C and an internal transmittance per mm in thickness within a wavelength region of from 200 to 700 nm, i.e. T 200 to 700, of at…
The present invention provides a TiO 2 -SiO 2 glass whose coefficient of linear thermal expansion in the range of the time of irradiation with EUV light is substantially zero when used as an optical member of an exposure tool for EUVL and which has extremely high surface…
The present invention relates to a non-alkali glass which has a strain point of 735˚C or higher, an average thermal expansion coefficient of 30×10 -7 to 40×10 -7 /˚C at 50 to 350˚C, a temperature (T 2 ) at which the viscosity of the glass becomes 10 2 dPa·s of 1710˚C or lower, a…
The present invention provides a tempered glass plate having a low thermal expansion coefficient, high surface compressive stress by physical strengthening, low density, and excellent abrasion resistance. The tempered glass plate has the following composition, in mass percent,…
The present invention is to provide an optical member for Extreme Ultra-Violet Lithography which is used for a reflective type mask, a mirror, etc. for EUVL and has excellent flatness and surface roughness on an optical surface thereof and in which chamfer parts are inhibited…
A TiO 2 -containing silica glass having a TiO 2 content of 7.5 to 12 mass% and a fictive temperature of 1000˚C or higher, wherein the temperature at which the linear thermal expansion coefficient of the silica glass becomes 0 ppb/°C falls within the range from 40 to 110°C.
Disclosed is silica glass containing TiO 2 , which contains TiO 2 in an amount of 5-10% by mass, while containing at least one of B 2 O 3 , P 2 O 5 or S in an amount of from 50 ppb by mass to 5% by mass in total.
The present invention relates to a TiO 2 -containing silica glass containing TiO 2 in an amount of from 5 to 10 mass % and at least one of B 2 O 3 , P 2 O 5 and S in an amount of from 50 ppb by mass to 5 mass % in terms of the total content.