A plasma display panel comprising mutually opposing substrates and barrier ribs formed between adjacent pixels of a display between the substrates, wherein the barrier ribs are made of a fired product of a glass ceramic composition consisting essentially of a glass powder of P 2…
Ito Setsuro
A glass composition for a substrate consisting essentially of from 52 to 62 wt % of SiO2, from 5 to 12 wt % of Al2O3, from 0 to 4 wt % of MgO, from 3 to 5.5 wt % of CaO, from 6 to 9 wt % of SrO, from 0 to 13 wt % of BaO, from 17 to 27 wt % of MgO+CaO+SrO+BaO, from 7 to 14 wt %…
An optical amplifying glass comprising a matrix glass and, added thereto, from 0.01 to 10 wt % of Er, characterized in that said matrix glass substantially comprises, as represented by mol %, 20 to 80 of Bi2O3, 0 to 74.89 of B2O3, 0 to 79.99 of SiO2, 0.01 to 10 of CeO2, 0 to 50…
A method for preparing a mayenite type compound having been imparted with electroconductivity is provided. A method for preparing an electroconductive mayenite type compound, which comprises melting a raw material containing Al and at least one selected from the group of Ca and…
A process by which a conductive mayenite compound having satisfactory properties can be easily, stably, and inexpensively obtained without the need of expensive equipment, high-temperature or long-term reaction, or complicated reaction control. The process for producing a…
A process for inexpensively mass-producing a conductive mayenite compound having satisfactory properties without the need of expensive equipment or complicated control; and a mayenite compound obtained by the process. The process for producing a conductive mayenite compound…
An optical amplifying glass comprising a matrix glass and from 0.001 to 10% by mass percentage of Tm doped to the matrix glass, wherein the matrix glass contains from 15 to 80 mol % of Bi2O3 and further contains at least one component selected from the group consisting of SiO2,…
An optical amplifier glass comprising a matrix glass containing Bi2O3 and at least one of Al2O3 and Ga2O3, and Er doped to the matrix glass, wherein from 0.01 to 10% by mass percentage of Er is doped to the matrix glass which has a total content of Al2O3 and Ga2O3 of at least…
To provide a method for preparing a mayenite type compound having electroconductivity imparted. A method for preparing an electroconductive mayenite type compound, which comprises melting a raw material containing Al and at least one element selected from the group consisting of…
An optical amplifying glass having Er doped in an amount of from 0.01 to 10% as represented by mass percentage to a matrix glass comprising, by mol %, BiO 2 : 20 to 80, B 2 O 3 +SiO 2 : 5 to 75, Ga 2 O 3 +WO 3 +TeO 2 : 0.1 to 35, Al 2 O 3 ≦10, GeO 2 ≦30, TiO 2 ≦30, and SnO 2…
An optical amplifying glass having Er doped in an amount of from 0.01 to 10% as represented by mass percentage to a matrix glass comprising, by mol %, BiO2: 20 to 80, B2O3+SiO2: 5 to 75, Ga2O3+WO3+TeO2: 0.1 to 35, Al2O3<=10, GEO2<=30, TIO2<=30, AND SNO2<=30, and…
An electron emitter, a field emission display unit, a cold cathode fluorescent tube and a flat type lighting device that use a low-cost, mass-producible electron emitting material. Myenite (calcium alminosilicate) type compound conductive powder, containing at least 50 mol% of…
A light-amplifying glass comprising a matrix glass and, added thereto, 0.01 to 10 wt % of Er, characterized in that said matrix glass substantially comprises 20 to 80 % of Bi2O3, 0 to 74.8 % of B2O3, 0 to 79.99 % of SiO2, 0.01 to 10 % of CeO2, 0 to 50 % of Li2O, 0 to 50 % of…
An optical amplifying glass comprising a matrix glass and from 0.001 to 10% by mass percentage of Tm doped to the matrix glass, wherein the matrix glass contains from 15 to 80 mol % of Bi 2 O 3 and further contains at least one component selected from the group consisting of SiO…
A method for producing a glass-ceramic article, which comprises crystallizing a glass article consisting essentially of from 40 to 60% by weight of SiO₂, from 13 to 19% by weight of Al₂O₃, from 0 to 6% by weight of B₂O₃, from 8 to 16% by weight of MgO, from 2 to 6% by weight of…
A chemically stable plasma display panel (PDP) exhibiting good discharge characteristics such as discharge efficiency or discharge lag while saving power. The plasma display panel comprises a front substrate and a back substrate facing each other through a discharge space, a…
Provided is an organic electroluminescence element that is characterized by: the provision of an anode, a light-emitting layer, and a cathode in this order; an electron injection layer being arranged between the light-emitting layer and the cathode; and by the electrode…
A glass composition for a substrate comprising from 52 to 62 wt% of SiO 2 , from 5 to 12 wt% of Aℓ 2 O 3 , from 0 to 4 wt% of MgO, from 3 to 5.5 wt% of CaO, from 6 to 9 wt% of SrO, from 0 to 13 wt % of BaO, from 17 to 27 wt% of MgO+CaO+SrO+BaO, from 7 to 14 wt% of Li 2 O+Na 2…
An optical amplifier glass comprising a matrix glass containing Bi 2 O 3 and at least one of Al 2 O 3 and Ga 2 O 3 , and Er doped to the matrix glass, wherein from 0.01 to 10% by mass percentage of Er is doped to the matrix glass which has a total content of Al 2 O 3 and Ga 2 O…
For a PDP, a panel having favorable discharge properties such a high discharge efficiency and a short discharge delay, being chemically stable and capable of electric power saving, is desired. A plasma display panel comprising a front substrate and a rear substrate facing each…
A light emitting device including an organic electroluminescence element is provided. The light emitting device may be a display device or a lighting device. The organic electroluminescence element includes an anode, a light emitting layer, and a cathode that are arranged in…
A light-amplifying glass which comprises: a matrix glass comprising 20 to 80 mol% Bi2O3, 5 to 75 mol% B2O3 + SiO2, 0.1 to 35 mol% Ga2O3 + WO3 + TeO2, up to 10 mol% Al2O3, up to 30 mol% GeO2, up to 30 mol% TiO2, and up to 30 mol% SnO2 and containing no CeO2; and 0.01 to 10 wt.%…
An optical amplifying glass comprising a matrix glass and, added thereto, from 0.01 to 10 wt% of Er, characterized in that said matrix glass substantially comprises, as represented by mol%, 20 to 80 of Bi 2 O 3 , 0 to 74.89 of B 2 O 3 , 0 to 79.99 of SiO 2 , 0.01 to 10 of CeO 2…
A glass substantially comprising 6-55% of Bi2O3, 10-70% of SiO2, 3-40% of P2O5, 5-30% of Li2O+Na2O+K2O+Rb2O+Fr2O, 0-40% of Al2O3, 0-30% of MgO+CaO+SrO+BaO+ZnO, 0-20% of B2O3, 0-20% of GeO2, 0-20% of TiO2+ZrO2+SnO2+Y2O, and 0-10% of CeO2. An optical waveguide manufacturing method…
Novel method and apparatus for chamfering a glass substrate are provided for improving productivity by improving bending strength and shock strength of an end plane of the glass substrate and by preventing breakage and chipping of the glass substrate in a glass substrate…