A process for producing terpolymers of propylene, comprising: a) feeding into a slurry reactor a reaction mixture containing 50-85 wt.% of propylene, 1-10 wt.% of ethylene, 15-40 wt.% of another C4-C8 alpha-olefin, a catalyst system maintaining olefin polymerization at said…
Ackermans Nina
Terpolymer of propylene, ethylene and C 4 to C 8 α-olefin with good barrier properties and processing properties, wherein the amount of propylene in said terpolymer is at least 94 percent by weight and the melting temperature of said terpolymer is more than 140° C.
Melt-blown fiber having an average diameter of not more than 5.0 μm, said fiber comprises at least 85 wt.-% of a propylene copolymer, wherein • said melt blown fiber and/or said propylene copolymer has/have a melt flow rate MFR 2 (230 °C) measured according to ISO 1133 of at…
Melt-blown fiber having an average diameter of not more than 5.0 μm, said fiber comprises at least 85 wt.-% of a propylene copolymer, wherein • said melt blown fiber and/or said propylene copolymer has/have a melt flow rate MFR 2 (230° C.) measured according to ISO 1133 of at…
The invention relates to a multilayer film, where at least one exterior layer comprises 90-99.9 wt% of a polypropylene composition, which is comprised of a propylene random copolymer and 0.1 - 10.0 wt% of a propylene homopolymer having an MFR > 100 g/10 min (230°C, 2.16 kg).
Terpolymer of propylene, ethylene and C4 to C8 α-olefin with good barrier properties and processing properties, wherein the amount of propylene in said terpolymer is at least 94wt.-% and the melting temperature of said terpolymer is more than 140°C.
The invention relates to a stabilised polypropylene composition, having excellent processing stability as well as long term stability, which comprises a lactone antioxidant, an antioxidant having a melting point ≥ 200 0C and a hindered amine light stabiliser.
A multi-layer biaxially oriented polymer film comprising a core layer (CL) and at least one sealing layer (SL), · said sealing layer(s) (SL) comprise(s) a propylene copolymer composition (P) having a comonomer content in the range of 3.0 to 8.0 wt.-%, the comonomers are C 5 to C…
The present invention relates to a composition, in particular to a polypropylene composition, and articles thereof, having an optimal balance between mechanical properties and transparency and thus the composition is particular suitable for packaging applications.
The present invention is directed to a thermal vaporization process for coating of polyolefin fibres with a metal, wherein said process comprises the following steps: inserting a polyolefin fibre or a sample of polyolefin fibres into a metallisation chamber comprising a heating…
Coated nonwoven fabric comprising a nonwoven fabric layer and a coating, said coating comprises a polymer having a branching index g′ of equal or below 0.9.
A multi-layer biaxially oriented polymer film comprising a core layer (CL) and at least one sealing layer (SL), said sealing layer(s) (SL) comprise(s) a propylene copolymer composition (P) having a comonomer content in the range of 3.0 to 8.0 wt.-%, the comonomers are C 5 to C…
A multi-layer biaxially oriented polymer film comprising a core layer (CL) and at least one sealing layer (SL), said sealing layer(s) (SL) comprise(s) a propylene copolymer composition (P) having a comonomer content in the range of 3.0 to 8.0 wt.-%, the comonomers are C5 to C12…
Melt-blown fiber having an average diameter of not more than 5.0 μm, said fiber comprises at least 85 wt.-% of a propylene copolymer, wherein •said melt blown fiber and/or said propylene copolymer has/have a melt flow rate MFR 2 (230° C.) measured according to ISO 1133 of at…
Coated nonwoven fabric comprising a nonwoven fabric layer and a coating, said coating comprises a polymer having a branching index g′ of equal or below 0.9.
The present invention relates to an article comprising a polymer composition comprising (A) a polyolefin matrix, and (B) a nanofiller dispersed in component (A), which composition has been stretched in at least one direction, to a process for the production of an article…
Melt-blown fiber having an average diameter of not more than 5.0 μm, said fiber comprises at least 85 wt.-% of a propylene copolymer, wherein • said melt blown fiber and/or said propylene copolymer has/have a melt flow rate MFR 2 (230 °C) measured according to ISO 1133 of at…
Coated nonwoven fabric comprising a nonwoven fabric layer and a coating, said coating comprises a polymer having a branching index g' of equal or below 0.9.