Terpolymer of propylene, ethylene and C 4 to C 8 α-olefin with good barrier properties and processing properties, wherein the amount of propylene in said terpolymer is at least 94 percent by weight and the melting temperature of said terpolymer is more than 140° C.
Assignee / Organization
De Ryck Mark
25Total Forward Citations
2Indexed Patents
12Avg Citations / Patent
2Portfolio H-Index
Terpolymer of propylene, ethylene and C4 to C8 α-olefin with good barrier properties and processing properties, wherein the amount of propylene in said terpolymer is at least 94wt.-% and the melting temperature of said terpolymer is more than 140°C.