Melt blown fiber
Abstract
Melt-blown fiber having an average diameter of not more than 5.0 μm, said fiber comprises at least 85 wt.-% of a propylene copolymer, wherein •said melt blown fiber and/or said propylene copolymer has/have a melt flow rate MFR 2 (230° C.) measured according to ISO 1133 of at least 200 g/10 min, •said propylene copolymer has a comonomer content of 0.5 to 5.5 wt.-%, the comonmers are ethylene and/or at least one C 4 to C 20 α-olefin selected from the group consisting of 1-butene, 1-pentene, 1-hexene, 1-heptene, and 1-octene, •the propylene copolymer has <2,1> regiodefects of not more than 0.4 mol.-% determined by 13 C-spectroscopy, and •said melt blown fiber and/or said propylene copolymer fulfill(s) the equation (1). wherein Tm [° C.] is the melting temperature [given in ° C.] of melt blown fiber said and/or of said propylene copolymer measured according to ISO 11357-3, C2 [wt %] is the amount [given in weight percentage] of comonomers within said melt blown fiber and/or within said propylene copolymer determined with Fourier transform infrared spectroscopy (FTIR). Tm [ ° C . ] [ ° C . ] ≥ 160 - C
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Melt-blown fiber having an average diameter of not more than 5.0 μm, said fiber comprises at least 85 wt.-% of a propylene copolymer, wherein said propylene copolymer is the only polymer in the melt-blown fiber, and wherein further (a) said melt blown fiber and/or said propylene copolymer has/have a melt flow rate MFR 2 (230° C.) measured according to ISO 1133 of at least 200 g/10 min, (b) said propylene copolymer has a comonomer content of 0.5 to 5.5 wt.-%, the comonmers are ethylene and/or at least one C 4 to C 20 α-olefin selected from the group consisting of 1-butene, 1-pentene, 1-hexen
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
References Cited — Backward Prior Art (17)
Non-Patent Literature (5)
- Antti Tynys, et al., Propylene Polymerisations with novel heterogeneous combination metallocene catalyst systems, Polymer, 2007, pp. 1893-1902, vol. 48, Elsevier Ltd.
- C.H. Stephens, et al., Comparison of Propylene/Ethylene Copolymers Prepared with Different Catalysts, Journal of Applied Polymer Science, 2006, pp. 1651-1658, vol. 100, Wiley Periodicals, Inc.
- Claudio De Rosa, Finizia Auriemma, Odda Ruiz De Ballesteros, Luigi Resconi & Isabella Camurati, Tailoring the Physical Properties of Isotactic Polypropylene through Incorporation of Comonomers and the Precise Control of Stereo- and Regioregularity by Metallocene Catalysts, Chemical of Materials, 200
- International Search Report and Written Opinion for European International Application No. PCT/EP2011/050676 Filed Jan. 19, 2011.
- Mario Hoyos, Pilar Tiemblo & Jose Manuel Gomez-Elvira, Effect of microstructure on the thermo-oxidation of solid isotactic polypropylene-based polyolefins, Science and Technology of Advance materials, 2008, pp. 1-13, vol. 9, National Institute for Materials in UK.