Nickel composite hydroxide and production method thereof, cathode active material for a non-aqueous electrolyte secondary battery and production method thereof, and a nonaqueous electrolyte secondary battery
Abstract
Provided is a cathode active material for a non-aqueous electrolyte secondary battery that has a uniform particle size and high packing density, and that is capable of increased battery capacity and improved coulomb efficiency. When producing a nickel composite hydroxide that is a precursor to the cathode active material by supplying an aqueous solution that includes at least a nickel salt, a neutralizing agent and a complexing agent into a reaction vessel while stirring and performing a crystallization reaction, a nickel composite hydroxide slurry is obtained while controlling the ratio of the average particle size per volume of secondary particles of nickel composite hydroxide that is generated inside the reaction vessel with respect to the average particle size per volume of secondary particles of nickel composite hydroxide that is finally obtained so as to be 0.2 to 0.6, after which, while keeping the amount of slurry constant and continuously removing only the liquid component, the crystallization reaction is continued until the average particle size per volume of secondary particles of the nickel composite hydroxide becomes 8.0 μm to 50.0 μm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 6.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A nickel composite hydroxide that is a precursor to a cathode active material for a non-aqueous electrolyte secondary battery, and comprising secondary particles of nickel composite hydroxide that are formed by an aggregation of plural primary particles, the secondary particles having an average particle size per volume (MV) that is within a range of 9.0 μm to 50.0 μm, and (D90−D10)/MV that indicates a particle size distribution per volume that is less than 0.5.
- Claim 2Depends on #1
The nickel composite hydroxide according to claim 1 wherein (D90−D10)/MV is 0.30 or more but less than 0.5.
- Claim 3Depends on #1
The nickel composite hydroxide according to claim 1 that was obtained by a production method for producing a nickel composite hydroxide that is a precursor to a cathode active material for a non-aqueous electrolyte secondary battery; the
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (24)
Non-Patent Literature (5)
- 103(c) Statement for WIPO WO 2011/067935 in association for US 2012/0270107 dated Aug. 25, 2016.
- Extended European Search Report issued by the European Patent Office in counterpart foreign Application No. 13751304.0 on Oct. 23, 2015, 9 pages.
- International Search Report and Written Opinion of the International Search Authority in counterpart PCT Application No. JP 2013/054595 dated Feb. 23, 2013, 11 pages, and English translation thereof.
- International Search Report re PCT Application No. JP 2013/054595 dated Feb. 23, 2013, 11 pages.
- Nakahara et al., Journal of Power Sources, vol. 117, 2003, pp. 131-136.