Nickel composite hydroxide and manufacturing method thereof, cathode active material for nonaqueous-electrolyte secondary battery and manufacturing method thereof, and nonaqueous-electrolyte secondary battery
Abstract
Provided are a cathode active material having a suitable particle size and high uniformity, and a nickel composite hydroxide as a precursor of the cathode active material. When obtaining nickel composite hydroxide by a crystallization reaction, nucleation is performed by controlling a nucleation aqueous solution that includes a metal compound, which includes nickel, and an ammonium ion donor so that the pH value at a standard solution temperature of 25° C. becomes 12.0 to 14.0, after which, particles are grown by controlling a particle growth aqueous solution that includes the formed nuclei so that the pH value at a standard solution temperature of 25° C. becomes 10.5 to 12.0, and so that the pH value is lower than the pH value during nucleation. The crystallization reaction is performed in a non-oxidizing atmosphere at least in a range after the processing time exceeds at least 40% of the total time of the particle growth process from the start of the particle growth process where the oxygen concentration is 1 volume % or less, and with controlling an agitation power requirement per unit volume into a range of 0.5 kW/m 3 to 4 kW/m 3 at least during the nucleation process.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A nickel composite hydroxide that is a precursor to a cathode active material for a nonaqueous-electrolyte secondary battery is expressed by the general expression: Ni x Mn y Co z M t (OH) 2+a (x+y+z+t=1, 0.3≤x≤0.7, 0.1≤y≤0.55, 0≤z≤0.4, 0≤t≤0.1, 0≤a≤0.5, and M is one or more kind of additional element that is selected from among Al, Ti, V, Cr, Zr, Nb, Mo, Hf, Ta and W), and is nearly spherical secondary particles that are formed by plural primary particles clumping together; the secondary particles having an average particle size that is greater than 7 μm and less than or equal to 15 μM, and
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (17)
Non-Patent Literature (5)
- Hashimoto (JP2008-147068, Machine Translation), Dec. 2008.
- International Search Report and Written Opinion dated Jul. 17, 2012, from the corresponding PCT/JP2012/059101.
- JP2008-147068, Human Translation, Jun. 2008.
- Lee "Synthetic optimization of Li[Ni1/3Co1/3Mn1/3]O2 via co-precipitation", Electrochimica Acta 50 (2004) 939-948, Sep. 11, 2004.
- Lee, Synthetic optimization of Li[Ni1/3Co1/3Mn1/3]O2 via co-precipitation, Electrochimica Acta 50 (2004) 939-948, Sep. 2004.