Patents
US 11,545,663 B2#153880579 Most CitedActiveUnited States (USPTO)Utility

Nickel composite hydroxide and manufacturing method thereof, cathode active material for nonaqueos-electrolyte secondary battery and manufacturing method thereof, and nonaqueous-electrolyte secondary battery

0Forward Citations (#153880579 Global)
0.0/yrCitation Velocity (#153880579 Global)
0.56Citation PageRank (#153880579 Global)
18Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Provided are a cathode active material having a suitable particle size and high uniformity, and a nickel composite hydroxide as a precursor of the cathode active material. When obtaining nickel composite hydroxide by a crystallization reaction, nucleation is performed by controlling a nucleation aqueous solution that includes a metal compound, which includes nickel, and an ammonium ion donor so that the pH value at a standard solution temperature of 25° C. becomes 12.0 to 14.0, after which, particles are grown by controlling a particle growth aqueous solution that includes the formed nuclei so that the pH value at a standard solution temperature of 25° C. becomes 10.5 to 12.0, and so that the pH value is lower than the pH value during nucleation. The crystallization reaction is performed in a non-oxidizing atmosphere at least in a range after the processing time exceeds at least 40% of the total time of the particle growth process from the start of the particle growth process where the oxygen concentration is 1 volume % or less, and with controlling an agitation power requirement per unit volume into a range of 0.5 kW/m3 to 4 kW/m3 at least during the nucleation process.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A cathode active material for a nonaqueous-electrolyte secondary battery that is essentially composed of a lithium nickel composite oxide that is expressed by the general expression: L 1+u Ni x Mn y Co z M t O 2 (−0.05≤u≤0.50, x+y+z+t=1, 0.3≤x, 0≤y≤0.55, 0≤z≤0.4, 0≤t≤0.1, and M is one or more kind of additional element that is selected from among Al, Ti, V, Cr, Zr, Nb, Mo, Hf, Ta and W), and has a hexagonal crystal structure; the lithium nickel composite oxide composed of substantially spherical secondary particles that are formed of sintered primary particles that clump together, wherein an a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
JP H05290832 AManufacture of positive electrode for lithium secondary battery—15
JP 2003086182 APositive electrode active material, method of manufacture, and nonaqueous electrolyte secondary battery—63
KR 20040007356 AManufacturing process of cathodes materials of lithium second battery, the reactor used therein and cathodes materials of lithium second battery manufactured thereby—51
JP 2004193115 APositive electrode active material for non-aqueous electrolyte secondary battery and non-aqueous electrolyte secondary battery—76
JP 2004210560 AManganese-nickel mixed hydroxide particle—34
JP 2004253174 APositive pole active material for nonaqueous electrolytic secondary battery—83
JP 2005008461 AMethod for producing compound oxide, compound oxide, and battery—27
JP 2008147068 ALithium composite oxide for nonaqueous electrolyte secondary battery—138
US 2009029253 A1Positive electrode material for lithium ion battery with nonaqueous electrolyte, and battery using the same—110
US 2009302267 A1Inorganic Compounds—25
KR 20100084621 AGranulated powder of transition metal compound for raw material for positive electrode active material of lithium secondary battery, and method for producing the same—8
US 2010196761 A1Granular powder of transition metal compound as raw material for cathode active material for lithium secondary battery, and method for its production—23
JP 2010192424 ACathode active material for nonaqueous electrolyte secondary battery, its manufacturing method, and nonaqueous electrolyte secondary battery using the same—75
WO 2011/067937 A1Nickel complex hydroxide particles and nonaqueous electrolyte secondary battery—42
US 2012270107 A1Nickel-cobalt-manganese complex hydroxide particles and method for producing same, positive electrode active material for nonaqueous electrolyte secondary battery and method for producing same, and nonaqueous electrolyte secondary battery—87
US 2012276454 A1Nickel complex hydroxide particles and nonaqueous electrolyte secondary battery—46
US 8,765,305 B2Cathode active material for lithium secondary battery, process for preparing the same and reactor for use in the same process20145
US 9,685,656 B2Nickel composite hydroxide and production method thereof, cathode active material for a non-aqueous electrolyte secondary battery and production method thereof, and a nonaqueous electrolyte secondary battery20176

Non-Patent Literature (5)

  • Final Office Action dated Feb. 27, 2017, from the corresponding U.S. Appl. No. 14/124,418.
  • Final Office Action dated Mar. 9, 2018, from the corresponding U.S. Appl. No. 14/124,418.
  • Final Office Action dated May 18, 2020, from the corresponding U.S. Appl. No. 15/892,681.