Patents
US 9,302,939 B2#64848079 Most CitedActiveUnited States (USPTO)Utility

Method for manufacturing stone material using molten slag

0Forward Citations (#64848079 Global)
0.0/yrCitation Velocity (#64848079 Global)
0.56Citation PageRank (#64848079 Global)
36Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for manufacturing a reconstituted stone raw material by using a molten slag includes: controlling a temperature of the molten slag at 1400° C.-1500° C., and performing a cast-molding process on the molten slag; and maintaining the cast-molded slag at a temperature of 800° C.-1000° C. for 1-5 hours in a non-reducing atmosphere, and then gradually cooling the cast-molded slag to a room temperature within 2-5 hours to obtain the reconstituted stone raw material. An energy-saving and efficient method for comprehensively utilizing the blast furnace slag is provided. The produced reconstituted stone raw material has such characteristics as stable color quality, abrasion resistance, pressure resistance, strong adhesiveness, low coefficient of expansion and low shrinkage ratio.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 36 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a reconstituted stone raw material by using a molten slag, comprising steps performed sequentially: introducing the molten slag into a pool for preserving heat; maintaining a temperature of the molten slag in the pool at 1450-1600° C.; adjusting a composition and/or a color of the molten slag in the pool according to requirements of a resulting product by adding color modifier; wherein the molten slag is directly discharged from a metallurgy reactor or is a remelted slag, wherein the molten slag includes 10-40 wt % of Al 2 O 3 , 5-25 wt % of MgO, 10-50 wt % of SiO 2

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (36)

PatentTitleYearCitations
US 3,133,804 AApparatus for treating molten ash or slag196423
US 3,223,508 AMixing device for admixing additives to a melt19654
US 3,531,270 AMolten steel slag handling method and apparatus19704
JP S5573804 AProduction of colored spherical blast furnace slag—3
JP S55140725 AManufacture of slag wool using steel making slag as starting material—8
US 4,376,805 AFused cast blocks based on refractory oxides and having a steel member embedded therein198311
US 4,918,034 AReservoir feed method of making ceramic composite structures and structures made thereby199011
US 4,943,398 AMethod for manufacturing a fused cast refractory199010
CN 1,065,646 ASlag microcrystalline glass directly made by industry furnace molten cinder—25
JP H0564779 AMolten slag container and method and apparatus for producing hard aggregate out of waste as raw material using the container—11
US 5,361,841 ADrilling and cementing with blast furnace slag/polyalcohol fluid199440
US 5,626,646 AMethod of recovering metals and producing a secondary slag from base metal smelter slag19978
US 5,865,872 AMethod of recovering metals and producing a secondary slag from base metal smelter slag199919
US 6,311,522 B1Process for casting and forming slag products20016
US 6,592,640 B1Fused Al2O3-Y2O3 eutectic abrasive particles, abrasive articles, and methods of making and using the same200312
US 6,596,041 B2Fused AL2O3-MgO-rare earth oxide eutectic abrasive particles, abrasive articles, and methods of making and using the same20037
US 2005051057 A1Thermal protective coating for ceramic surfaces—52
CN 1,923,741 ANanometer composite gel material and preparation method thereof—13
CN 101,020,968 AProcess of comprehensively utilizing high temperature nickel smelting slag—46
US 2008017077 A1Slag concrete manufactured aggregate—51
CN 101,121,948 AMethod for processing iron-fining furnace slag without water—7
CN 101,259,987 AMethod for preparing microcrystalline glass by using blast furnace slag—29
CN 101,289,332 ALow-temperature ceramic foam material and production method thereof—57
CN 101,318,787 AProcess and method for converting waste slag wholly of aluminum industry into ecological building material—27
CN 101,323,503 AMethod for preparing microcrystalline foamed glass by titanium-containing blast furnace slag—26
CN 101,372,405 ABuilding material and method of manufacturing the same—22
CN 101,559,953 AMethod for using high-temperature liquid silicon manganese alloy slag as raw material to produce cast stone—18
US 2010035037 A1Method of fabricating an ltm perovskite product—5
CN 101,698,568 AMethod for preparing jade type microcrystalline glass with high-temperature furnace slag—27

Non-Patent Literature (1)

  • International Search Report for PCT/CN2011/079894, English translation attached to original, Both completed by the Chinese Patent Office on Dec. 5, 2011, All together 8 Pages.