US 2013167586 A1#31885949 Most Cited · 3 citations0.2/yr · PR 1.13PendingUS · Application
Method for manufacturing plate inorganic nonmetal material using molten slag

A method for manufacturing a plate inorganic nonmetal material by using a molten slag by introducing the molten slag into a pool for preserving heat and modifying, wherein a temperature of the molten slag is 1450° C.-1600° C., and modifying a viscosity and/or a color of the…

US 2013175736 A1#35430212 Most Cited · 2 citations0.1/yr · PR 1.33PendingUS · Application
Method for manufacturing stone material using molten slag

A method for manufacturing a reconstituted stone raw material by using a molten slag includes: controlling a temperature of the molten slag at 1400° C.-1500° C., and performing a cast-molding process on the molten slag; and maintaining the cast-molded slag at a temperature of…

US 2013161854 A1#58376271 Most Cited · 1 citations0.1/yr · PR 0.78PendingUS · Application
Method for manufacturing foam material using molten slag

A method for manufacturing a foam material by using a molten slag includes: introducing the molten slag maintained at 1400° C.-1500° C. into a pool for preserving heat, and adding a viscosity modifier and/or a color modifier to the molten slag to adjust a viscosity and/or a…

US 8,991,212 B2#89955203 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Method for manufacturing plate inorganic nonmetal material using molten slag
Inventors: Wang Qingtao, Yu Xianjin, Zhao Xin, Gong Benkui, Wei ZhenxiaAssignee: Wang Qingtao, Yu XianjinFiled 2011-09-20 · Granted 2015-03-31

A method for manufacturing a plate inorganic nonmetal material by using a molten slag by introducing the molten slag into a pool for preserving heat and modifying, wherein a temperature of the molten slag is 1450° C.-1600° C., and modifying a viscosity and/or a color of the…

US 9,139,471 B2#96177942 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Method for manufacturing foam material using molten slag
Inventors: Wang Qingtao, Yu Xianjin, Zhao Xin, Gong Benkui, Wei ZhenxiaAssignee: Wang Qingtao, Yu XianjinFiled 2011-09-20 · Granted 2015-09-22

A method for manufacturing a foam material by using a molten slag includes: introducing the molten slag maintained at 1400° C.-1500° C. into a pool for preserving heat, and adding a viscosity modifier and/or a color modifier to the molten slag to adjust a viscosity and/or a…

US 9,302,939 B2#64848079 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Method for manufacturing stone material using molten slag
Inventors: Wang Qingtao, Yu Xianjin, Zhao Xin, Gong Benkui, Wei ZhenxiaAssignee: Wang Qingtao, Yu XianjinFiled 2011-09-20 · Granted 2016-04-05

A method for manufacturing a reconstituted stone raw material by using a molten slag includes: controlling a temperature of the molten slag at 1400° C.-1500° C., and performing a cast-molding process on the molten slag; and maintaining the cast-molded slag at a temperature of…

WO 2012/041172 A1#147420637 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method for manufacturing reductive stone material using molten slag

A method for manufacturing a reductive stone material using a molten slag. The method comprises these steps: controlling the molten slag at a temperature between 1,400°C and 1,500°C, and cast molding at a controlled temperature; thermally insulating the molded molten slag at a…

WO 2012/041173 A1#147975870 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method for manufacturing planar inorganic non-metallic material using molten slag

A method for manufacturing a planar inorganic non-metallic material using a molten slag. The method comprises these steps: feeding the molten slag into a thermal insulated conditioning pool and maintaining the temperature of the molten slag between 1,450°C and 1,600°C; modifying…

WO 2012/041174 A1#111800231 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method for manufacturing foam material by using molten slag

A method for manufacturing a foam material by using a molten slag. The method comprises these steps: feeding the molten slag into a thermal insulated conditioning pool and maintaining the temperature of the molten slag between 1,400°C and 1,500°C; on the basis of the…