Wei Zhenxia

8Total Forward Citations
69Indexed Patents
2Patent H-Index
US 2013167586 A1#31885949 Most Cited · 3 citations0.2/yr · PR 1.13PendingUS · Application
Method for manufacturing plate inorganic nonmetal material using molten slag

A method for manufacturing a plate inorganic nonmetal material by using a molten slag by introducing the molten slag into a pool for preserving heat and modifying, wherein a temperature of the molten slag is 1450° C.-1600° C., and modifying a viscosity and/or a color of the…

US 2013175736 A1#35430212 Most Cited · 2 citations0.1/yr · PR 1.33PendingUS · Application
Method for manufacturing stone material using molten slag

A method for manufacturing a reconstituted stone raw material by using a molten slag includes: controlling a temperature of the molten slag at 1400° C.-1500° C., and performing a cast-molding process on the molten slag; and maintaining the cast-molded slag at a temperature of…

EP 2,623,475 A1#53992115 Most Cited · 1 citations0.1/yr · PR 0.82PendingEP · Application
Method for manufacturing reductive stone material using molten slag

A method for manufacturing a reconstituted stone raw material by using a molten slag includes: controlling a temperature of the molten slag at 1400°C -1500°C, and performing a cast-molding process on the molten slag; and maintaining the cast-molded slag at a temperature of 800°C…

KR 20130062346 A#51380210 Most Cited · 1 citations0.1/yr · PR 0.85ActiveKR · Utility
Method for manufacturing stone material using molten slag

용융 슬래그를 이용하여 환원 석재 원료를 제조하는 방법에 있어서, 용융 슬래그의 온도를 1400℃-1500℃로 제어하여 온도제어 주조성형을 진행하는 단계와, 성형된 슬래그를 800℃-1000℃의 온도하에서 또한 비환원성 분위기 하에서 1-5시간 보온시킨 후, 2-5시간 내에 점차적으로 실온까지 온도를 낮추어 환원 석재원료를 얻는 단계를 포함한다. 당해 방법은 고로 슬래그의 종합 이용을 위해 에너지 절약 및 고효율적인 대책을 제공하였고, 제조해낸 환원 석재원료는 색상이 안정적이고, 마모에 견디며,…

US 2013161854 A1#58376271 Most Cited · 1 citations0.1/yr · PR 0.78PendingUS · Application
Method for manufacturing foam material using molten slag

A method for manufacturing a foam material by using a molten slag includes: introducing the molten slag maintained at 1400° C.-1500° C. into a pool for preserving heat, and adding a viscosity modifier and/or a color modifier to the molten slag to adjust a viscosity and/or a…

AR 083,106 A1#153474763 Most Cited · 0 citations0.0/yr · PR 0.56PendingAR · Application
Metodo para fabricar material inorganico no metalico en placa usando escoria fundida

La presente provee un método para fabricar un material inorgánico no metálico en placa usando una escoria fundida, el método comprende: introducir la escoria fundida dentro de una pileta para preservar el calor en donde una temperatura de la escoria fundida se mantiene a 1450ºC…

AR 084,481 A1#117422279 Most Cited · 0 citations0.0/yr · PR 0.56PendingAR · Application
Metodo para fabricar material de espuma usando escoria fundida

La presente provee un método para fabricar un material de espuma mediante el uso de una escoria fundida, que comprende: introducir la escoria fundida dentro de una pileta para preservar el calor y modificar, en donde una temperatura de la escoria fundida se mantiene a 1400ºC -…

AR 084,718 A1#151160682 Most Cited · 0 citations0.0/yr · PR 0.56PendingAR · Application
Metodo para fabricar material de piedra usando escoria fundida

La presente provee un método para fabricar una materia prima de piedra reconstituida usando una escoria fundida, el método comprende: controlar una temperatura de la escoria fundida a 1400ºC - 1500ºC, y llevar a cabo un proceso de moldeo por fundición sobre la escoria fundida; y…

AU 2011307776 A1#64489755 Most Cited · 0 citations0.0/yr · PR 0.56PendingAU · Application
Method for manufacturing reductive stone material using molten slag

A method for manufacturing a reductive stone material using a molten slag. The method comprises these steps: controlling the molten slag at a temperature between 1,400°C and 1,500°C, and cast molding at a controlled temperature; thermally insulating the molded molten slag at a…

AU 2011307776 B2#127582034 Most Cited · 0 citations0.0/yr · PR 0.56ActiveAU · Utility
Method for manufacturing reductive stone material using molten slag
Inventors: Wang Qingtao, Yu Xianjin, Zhao Xin, Gong Benkui, Wei ZhenxiaAssignee: Shandong Coking Group Co LtdFiled 2011-09-20 · Granted 2014-05-01

A method for manufacturing a reductive stone material using a molten slag. The method comprises these steps: controlling the molten slag at a temperature between 1,400°C and 1,500°C, and cast molding at a controlled temperature; thermally insulating the molded molten slag at a…

AU 2011307777 A1#112209193 Most Cited · 0 citations0.0/yr · PR 0.56PendingAU · Application
Method for manufacturing planar inorganic non-metallic material using molten slag

A method for manufacturing a planar inorganic non-metallic material using a molten slag. The method comprises these steps: feeding the molten slag into a thermal insulated conditioning pool and maintaining the temperature of the molten slag between 1,450°C and 1,600°C; modifying…

AU 2011307777 B2#137274452 Most Cited · 0 citations0.0/yr · PR 0.56ActiveAU · Utility
Method for manufacturing planar inorganic non-metallic material using molten slag
Inventors: Wang Qingtao, Yu Xianjin, Zhao Xin, Gong Benkui, Wei ZhenxiaAssignee: Shandong Coking Group Co LtdFiled 2011-09-20 · Granted 2014-02-20

A method for manufacturing a planar inorganic non-metallic material using a molten slag. The method comprises these steps: feeding the molten slag into a thermal insulated conditioning pool and maintaining the temperature of the molten slag between 1,450°C and 1,600°C; modifying…

AU 2011307778 A1#91024882 Most Cited · 0 citations0.0/yr · PR 0.56PendingAU · Application
Method for manufacturing foam material by using molten slag

A method for manufacturing a foam material by using a molten slag. The method comprises these steps: feeding the molten slag into a thermal insulated conditioning pool and maintaining the temperature of the molten slag between 1,400°C and 1,500°C; on the basis of the…

AU 2011307778 B2#87695573 Most Cited · 0 citations0.0/yr · PR 0.56ActiveAU · Utility
Method for manufacturing foam material by using molten slag
Inventors: Wang Qingtao, Yu Xianjin, Zhao Xin, Gong Benkui, Wei ZhenxiaAssignee: Shandong Coking Group Co LtdFiled 2011-09-20 · Granted 2014-04-17

A method for manufacturing a foam material by using a molten slag. The method comprises these steps: feeding the molten slag into a thermal insulated conditioning pool and maintaining the temperature of the molten slag between 1,400°C and 1,500°C; on the basis of the…

BR 112013004103 A2#131786405 Most Cited · 0 citations0.0/yr · PR 0.56PendingBR · Application
método para fabricação de material não metálico inorgânico em placa usando escória fundida

método para fabricação de material não metálico inorgânico em placa usando escória fundida. um método para a fabricação de um material não metálico inorgânico em placa por emprego de escória fundida inclui: introdução de escória fundida em um tanque para preservação do calor e…

BR 112013004237 A2#96748837 Most Cited · 0 citations0.0/yr · PR 0.56PendingBR · Application
método para fabricação de material de rocha usando escória fundida

método para fabricação de material de rocha usando escória fundida. um método para a fabricação de uma matéria prima de rocha reconstituída utilizando uma escória fundida inclui: controle da temperatura da escória fundida a 1.400<198>c-1.500<198>c e realização de um…

CA 2,806,286 A1#112747261 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Method for manufacturing stone material using molten slag

A method for manufacturing a reconstituted stone raw material by using a molten slag includes: controlling a temperature of the molten slag at 1400°C-1500°C, and performing a cast-molding process on the molten slag; and maintaining the cast-molded slag at a temperature of…

CA 2,806,286 C#131601843 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCA · Utility
Method for manufacturing stone material using molten slag
Inventors: Wang Qingtao, Yu Xianjin, Zhao Xin, Gong Benkui, Wei ZhenxiaAssignee: Shandong Coking Group Co LtdFiled 2011-09-20 · Granted 2015-02-10

A method for manufacturing a reconstituted stone raw material by using a molten slag includes: controlling a temperature of the molten slag at 1400°C-1500°C, and performing a cast-molding process on the molten slag; and maintaining the cast-molded slag at a temperature of…

CA 2,806,289 A1#77554063 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Method for manufacturing plate inorganic nonmetal material using molten slag

A method for manufacturing a planar inorganic non-metallic material using a molten slag. The method comprises these steps: feeding the molten slag into a thermal insulated conditioning pool and maintaining the temperature of the molten slag between 1,450°C and 1,600°C; modifying…

CA 2,806,289 C#116788686 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCA · Utility
Method for manufacturing plate inorganic nonmetal material using molten slag
Inventors: Wang Qingtao, Yu Xianjin, Zhao Xin, Gong Benkui, Wei ZhenxiaAssignee: Shandong Coking Group Co LtdFiled 2011-09-20 · Granted 2014-07-29

A method for manufacturing a plate inorganic nonmetal material by using a molten slag includes: introducing the molten slag into a pool for preserving heat and modifying, wherein a temperature of the molten slag is maintained at 1450 °C -1600°C, and modifying a viscosity and/or…

CA 2,806,292 A1#147176067 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Method for manufacturing foam material using molten slag

A method for manufacturing a foam material by using a molten slag includes: introducing the molten slag into a pool for preserving heat and modifying, wherein a temperature of the molten slag is maintained at 1400°C-1500°C, and adding a viscosity modifier and/or a color modifier…

CA 2,806,292 C#115062882 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCA · Utility
Method for manufacturing foam material using molten slag
Inventors: Wang Qingtao, Yu Xianjin, Zhao Xin, Gong Benkui, Wei ZhenxiaAssignee: Shandong Coking Group Co LtdFiled 2011-09-20 · Granted 2015-02-10

A method for manufacturing a foam material by using a molten slag includes: introducing the molten slag into a pool for preserving heat and modifying, wherein a temperature of the molten slag is maintained at 1400°C-1500°C, and adding a viscosity modifier and/or a color modifier…

CN 102,242,231 B#70647647 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Method for producing flat plate type inorganic non-metallic material by using molten slag

The invention provides a method for producing a flat-plate type inorganic non-metallic material by using molten slag, which is characterized by comprising the following steps: enabling the molten slag to enter a heat-preservation tempering pool, keeping the temperature of the…

CN 102,249,567 B#73870084 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Method for producing reduced stone raw material by using molten slag

The invention provides a method for producing a reduced stone raw material by using molten slag, which comprises the following steps: controlling the temperature of the molten slag to 1400-1500 ℃, and carrying out temperature-controlled casting molding; keeping the temperature…

CN 102,249,731 B#75460111 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Method for producing foam material by using molten slag

The present invention provides a method for producing a foamed material using molten slag, the method comprising the steps of: enabling the molten slag to enter a heat-preservation tempering pool, keeping the temperature of the slag at 1400-1500 ℃, and adding a color regulator…