US 9,280,688 B2#100678209 Most CitedActiveUnited States (USPTO)Utility

Apparatus and method for limiting and analyzing stress corrosion cracking in pressurized water reactors

0Forward Citations (#100678209 Global)
0.0/yrCitation Velocity (#100678209 Global)
0.56Citation PageRank (#100678209 Global)
19Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method to assess and predict pressurized water stress corrosion cracking in operational nuclear power plants and the effect of adding zinc compounds into a reactor coolant system of the nuclear power plant.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method to evaluate an effect of applying a zinc compound to a reactor coolant system of a pressurized water reactor, comprising: quantitatively assessing a pressurized water reactor stress corrosion cracking initiation rate of a candidate reactor coolant system through analysis of operational eddy current testing data and pressurized water stress corrosion cracking failure history using empirical relationships; determining an extent of damage to the candidate system; quantitatively assessing pressurized water stress corrosion cracking initiation benefit for high-concentration (>10 ppb) an

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
US 3,580,934 ACorrosion prevention with sodium silicate and soluble zinc salts197120
US 4,625,165 ATube inspection probe with rotating eddy current coil198637
US 4,756,874 AMinimization of radioactive material deposition in water-cooled nuclear reactors198821
US 4,950,449 AInhibition of radioactive cobalt deposition in water-cooled nuclear reactors199016
US 5,108,697 AInhibiting stress corrosion cracking in the primary coolant circuit of a nuclear reactor199223
US 5,171,515 AProcess for inhibiting corrosion in a pressurized water nuclear reactor199221
US 5,181,533 AControlled dispenser199330
US 5,600,691 ANoble metal doping or coating of crack interior for stress corrosion cracking protection of metals199719
US 5,818,893 AIn-situ palladium doping or coating of stainless steel surfaces199849
US 5,995,576 AInhibition of radioactive material deposition in primary coolant structure of nuclear power plant19999
WO 0,022,627 A1Application of noble metals to internal surfaces of operating boiling water reactors in the presence of zinc in reactor water—3
US 6,314,153 B1Process for introducing zinc into a water-containing component of the primary system of a nuclear power plant200117
US 6,415,010 B2Catalytic hydrogen peroxide decomposer in water-cooled reactors20029
US 2002118787 A1Noble metal catalysis for mitigation of corrosion, erosion and stress corrosion cracking in pressurized water reactor and related high temperature water environments—10
US 6,473,480 B1Method and apparatus for maintaining proper noble metal loading for a noble metal application process for water-cooled nuclear reactors200219
US 2002191731 A1Method for controlling zinc addition to power reactor—4
US 6,714,618 B1Temperature-based method for controlling the amount of metal applied to metal oxide surfaces to reduce corrosion and stress corrosion cracking200413
US 2005105670 A1Pressurized water reactor shutdown method—16
US 6,944,254 B2Pressurized water reactor shutdown method200513

Non-Patent Literature (5)

  • AcademicPress Dictionary of Science and Technology, "Solubility" (1992, 1996), credoreference.com/entry/3160396.
  • Andersen, P.L.et al., "Effects of Zinc Additions on the Crack Growth Rate of Sensitized Stainless Steel and Alloys 600 and 182 in 288° C. Water", Water Chemistry of Nuclear Reactor Systems 6, BNES, London, 1992, Paper No. 72.
  • Kawamura, H. et al., "Inhibitory Effect of Zinc Addition of High-Temperature Hydrogenated Water on Mill-Annealed and Prefilmed Alloy 600", Corrosion (2000), vol. 56:6, pp. 623-637.
  • Kawamura, H. et al., "The Effect of Zinc Addition to Simulated PWR Primary Water on the PWSCC Resistance, Crack Growth Rate and Surface Oxide Film Characteristics of Prefilmed Alloy 600", Corrosion 98, NACE International, Houston, 1998, Paper No. 141.
  • Palmer et al., "New Measurements of the Solubility of Metal Oxides at High Temperatures" Aqueous Systems at Elevated Temperatures and Pressures, ORNL 2004.