Patents
US 5,108,697 A#3377978 Most CitedExpiredUnited States (USPTO)Utility

Inhibiting stress corrosion cracking in the primary coolant circuit of a nuclear reactor

23Forward Citations (#3377978 Global)
0.7/yrCitation Velocity (#11148505 Global)
5.11Citation PageRank (#3196051 Global)
8Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A primary coolant circuit for cooling a nuclear reactor has wetted mechanically stressed nickel base alloy components such as Alloy 600 tubes in steam generators having oxidized surfaces comprising 1-10 w/o zinc, which tubes are inhibited against primary water stress corrosion cracking. The crack initiation times may be delayed by a factor of two in pressurized water nuclear reactors.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 23.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of inhibiting stress corrosion cracking in a pressurized water nuclear reactor, comprising the steps of: (a) circulating coolant water through the primary cooling circuit of a pressurized water nuclear reactor in contact with nickel base alloys comprising at least about 60 w/o nickel, about 13-30 w/o chromium and about 0.3-12 w/o iron, (b) maintaining the coolant water composition at about 1-2500 ppm boron, about 0.1-10 ppm lithium, and about 15-75 cc (STP) hydrogen/kg water, (c) maintaining the coolant water pH between about 5.2 and about 7.4 at 20° C. and conductivity betw

  2. Claim 2Depends on #1

    The method of claim 1, wherein the coolant water is maintained bet

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 23 total)

Non-Patent Literature (2)

  • Electric Power Research Institute Report 4447, Mar. 1986.
  • Electric Power Research Institute Report 6168, Jan. 1989.