Patents
US 9,040,440 B2#65856747 Most CitedActiveUnited States (USPTO)Utility

Method of toughening alumina

0Forward Citations (#65856747 Global)
0.0/yrCitation Velocity (#65856747 Global)
0.56Citation PageRank (#65856747 Global)
25Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present application is directed to a zirconia toughened alumina body and process for making the body. The process involves combining tetragonally stabilized ZrO 2 nanoparticles, Mg(OH) 2 particles and alumina powder into a mixture. All particles of the mixture are milled, formed into a green compact and then sintered. The final composition of the body includes α-Al 2 O 3 toughened with 0.5 to 2.5 weight percent ZrO 2 in a stabilized tetragonal form and 0.03 to 0.10 weight percent MgO. The composition results in an Al 2 O 3 body with a density less than 4.0 g/cc and strength greater than 50 kpsi.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating a ceramic, comprising the steps of: a) providing (i) crystalline α-Al 2 O 3 particles, (ii) 0.5-2.5 percent by weight crystalline ZrO 2 particles less than 0.1-microns and stabilized substantially in the tetragonal crystal structure, and (iii) 0.03-0.10 percent MgO by weight as Mg(OH) 2 particles; b) combining and milling all particles; c) forming a green compact; and d) sintering said green compact in a temperature range of 1637° C.-1660° C.

  2. Claim 2Depends on #1

    A method as recited in claim 1 , wherein during said providing step a) said percent by weight crystalline ZrO 2 particles is 1.0-2.0.

  3. Claim 3Depends on #1

    A method as recited in claim 1 , wherein during said providing step a) said percent MgO by weight is 0.03-0.05.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (25)

PatentTitleYearCitations
US 4,218,253 ASintered ceramic material of improved ductility198056
US 4,298,385 AHigh-strength ceramic bodies198157
US 4,316,964 AAl2 O3 /ZrO2 ceramic1982161
US 4,331,048 ACutting tip for metal-removing processing198240
US 4,501,818 AProcess for the preparation of ceramic powders198531
US 4,532,224 AComposite ceramic powders and a method of making the same198510
US 4,751,207 AAlumina-zirconia ceramic198822
US 4,772,576 AHigh density alumina zirconia ceramics and a process for production thereof198855
US 4,820,667 AHigh strength zirconia ceramic198937
US 4,900,701 AZirconia sintered body and process for the production thereof199014
US 4,952,536 AHigh strength Al2 O319907
US 5,032,555 AProcess for making zirconia-alumina199136
US 5,045,402 AZirconia toughening of glass-ceramic materials199127
US 5,130,210 AStabilized zirconia solid electrolyte and process for preparation thereof199243
US RE34028 EAlumina-zirconia ceramic199213
US 5,155,071 AFlame-produced partially stabilized zirconia powder199222
US 5,312,789 AAbrasive grits formed of ceramic, impregnation method of making the same and products made therewith199453
US 5,419,827 APartially stabilized zirconia and its application to electronical device199527
US 5,432,133 AProduction process of a sintered high-toughness alumina-based composite body19954
US 6,624,106 B2Alumina ceramic products200315
US 6,800,158 B2Method of making a sensor and the product produced therefrom200419
US 7,012,036 B2ZrO2-Al2O3 composite ceramic material and production method thereof200627
US 2006063661 A1Alumina ceramic products—14
US 7,148,167 B2Alumina/zirconia ceramics and method of producing the same200643
US 8,012,897 B2Alumina ceramic products20114