Patents
US 4,501,818 A#2095566 Most CitedExpiredUnited States (USPTO)Utility

Process for the preparation of ceramic powders

31Forward Citations (#2095566 Global)
0.8/yrCitation Velocity (#9754729 Global)
17.46Citation PageRank (#419140 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Sub-micron sized powders of the ceramic metal oxides such as zirconia, alumina, titania, etc. are produced by precipitation from substantially anhydrous solutions of salts of the corresponding metal(s) with substantially anhydrous solutions of alkali metal hydroxides. The precipitates are subsequently washed with water to remove any residual soluble salt and/or solvent, then are dried and usually calcined. The powders thus produced are readily sintered to high density ceramic bodies after conventional pressing into the desired shape. The process is especially suited to the production of zirconia powders, either pure or doped with conventional stabilizing oxides such as yttria. In a typical example, a zirconia powder doped with 5.4% by weight of yttria is prepared by adding a solution of zirconium tetrachloride and yttrium chloride in anhydrous ethanol to a solution of sodium hydroxide in anhydrous ethanol. After washing, drying at 105° C., and calcining at 500° C. for two hours, the powder is pressed at 5000 psi into a green body with a density of 1.46 Mg/m 3 . After one hour of sintering a 1600° C., the fired body has a density of 5.84 Mg/m 3 , which is 96% of the theoretical maxi

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 31.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of uniform, sub-micron size sinterable metal oxide ceramic powders, comprising the steps of: (a) forming a substantially anhydrous first solution of salts of all the metals whose oxides are present in said metal oxide ceramic powders in the proportions present therein and forming a substantially anhydrous second solution of alkali metal hydroxides in the amount stoichiometrically required to react with the metal content of said first solution; (b) adding said first solution to said second solution, so as to form without evidence of gellation a solid precipitate

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗