Zirconia sintered body and process for the production thereof
Abstract
A process for the production of a raw material used for the production of a zirconia sintered body is disclosed. A power containing principally zirconium compounds and a stabilizing agent is added to a solution or slurry containing at least one metal element selected from the group consisting of Mn, Fe, Co, Ni, Cu, and Zn. The stabilizing agent is Y 2 O 3 , CaO, MgO, CeO 2 , a yttrium compound, calcium compound, magnesium compound or cerium compound which can produce Y 2 O 3 , CaO, MgO, or CeO 2 by thermal decomposition. The selected metal element from the group will act as a coating on the zirconia sintered body.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 14.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In the production of a partially stabilized zirconia sintered body wherein the tetragonal phase content is sixty-five percent or more, the sintering temperature is 1100° C. to 1400° C. and the grain size is 0.5 μm or less, a process for the production of the sinterable raw material powder used for said production, said process comprising the steps of: (a) suspending a powder of a zirconium compound containing a stabilizing agent into a solution or slurry containing a compound of a transition metal element other than zirconium, the atomic ratio of said other transition metal element to zirconiu
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (14 of 14 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (2)
- Lange, F., "Transformation Toughening", J. Material Science 17 (1982) pp. 240-246.
- Lange, F., Transformation Toughening , J. Material Science 17 (1982) pp. 240 246.