Hybrid cement clinker and cement made from that clinker
Abstract
A hybrid cement clinker incorporates specific ranges of clinker phases and falls within specific modulus values as set forth and described in this document.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A cement clinker, comprising: about 35-41 weight percent C 3 S; about 10-15 weight percent C 2 S; about 14-16 weight percent C 4 A 3 S ; about 20-26 weight percent C 4 AF; about 4-6 weight percent CŚ; and about 0.7-0.85 weight percent CaF 2 ; fired at a temperature of about 1250-1300° C.
- Claim 2Depends on #1
The clinker of claim 1 having a lime adequate degree (LAD) modulus value of between 0.88 and 0.92, a ratio of silicates and aluminates (RSA) modulus value of between 1.0 and 1.7, a ratio of sulfoaluminates and ferroaluminates (RSF) modulus value of between 0.5 and 0.8, a sulfur excessive coefficient (SEC) modulus value of between 1.0 and 1.6 and a quantity of liquid phase (QLP) modulus value of between 0.095 and 0.105.
- Claim 3Depends on #1
The cement clinker of claim 1 incorporating stainless steel pickling sludge.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (26)
Non-Patent Literature (1)
- S. Giminez-Molina, et al.; "Phase relations in the system Ca2SiO4-CaO-CaSO4-CaF2 relevant to cement clinkering"; Advances in Cement Research, 1991/92, vol. 4, No. 14, pp. 81-86.