Very high early strength cement

33Forward Citations (#1898896 Global)
0.7/yrCitation Velocity (#10358559 Global)
11.08Citation PageRank (#894416 Global)
4Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A combination of a hydroxy polycarboxylic acid and sucrose improves the water-demand, setting, and compressive strength properties of a calcium sulfoaluminate cement to a greater degree than would be the case if the hypothetical cumulative effect of two admixtures were operative.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 33.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A hydraulic cement composition comprising from about 3.75% to about 40% of 3CaO.3Al 2 O 3 .CaSO 4 , from about 0.1% to about 5% of lime, from about 3% to about 35% of calcium sulfate, dicalcium silicate, from about 0.1% to about 2% of a hydroxy polycarboxylic acid, and from about 0.25% to about 4% of sucrose, said amounts being based upon the total dry weight of said composition.

  2. Claim 2Depends on #1

    The composition of claim 1 wherein the acid is citric acid.

  3. Claim 3Depends on #2

    The composition of claim 2 wherein the amount of citric acid is from about 0.25% to about 1%, the amount of sucrose is from about 0.25% to about 4%, and the sucrose to acid ratio is from about 1:1 to about 6:1.