Abstract

Disclosed are a hydraulic binder composition using rapidly-cooled steelmaking reduced slag powder and a method of preparing the same. More particularly, the rapidly-cooled steelmaking reduced slag (RC-LFS) powder is obtained by spraying and scattering gas at a high pressure and high speed onto electric furnace smelting reduction slag, which is one of the by-products generated during iron smelting performed in an ironworks, and quickly cooling and pulverizing the slag. The initial high hydration heat reaction and initial setting of the rapidly-cooled steelmaking reduced slag (RC-LFS) powder are delayed to ensure workability. A retardant and gypsum are mixed into the rapidly-cooled steelmaking reduced slag (RC-LFS) powder so as to activate the generation of needle-shaped ettringite and to thus develop the initial and long-term strength, and therefore the rapidly-cooled steelmaking reduced slag (RC-LFS) powder of the present invention can be used as a substitute for ordinary Portland cement.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of preparing a hydraulic binder composition for use as a substitute of ordinary Portland cement (OPC) by utilizing steelmaking reduction slag as starting material to produce the hydraulic binder composition, the method comprising: rapidly-cooling a steelmaking reduction slag from a temperature of 1,300-1,400° C. to 400-600° C. by spraying and scattering pressurized gas onto the steelmaking reduction slag for 5 to 10 seconds; pulverizing or comminuting the cooled steelmaking reduction slag into steelmaking reduction slag powder with a fineness of 3,000 cm 2 /g or higher; adding gypsum

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (23)

PatentTitleYearCitations
GB 821,741 AMethod and apparatus for the manufacture of a porous slag—7
JP S52130819 AMethod of manufacturing fiber glass reinforced cement boards—3
US 4,328,039 AHigh sulphate slag cement and method for manufacturing this cement198216
US 4,756,761 AMethods of making cementitious compositions from waste products198860
JP S63285114 AManufacture of zeolite l—5
JP S6437450 AQuick hardening cement composition—6
KR 900,000,033 B1Method for producing cement clinkers19903
JP H05294701 AQuick hardening cement compound—11
US 5,273,579 AQuick setting compositions199329
JP H06321607 AProduction of quick set composition—9
US 5,494,515 AMethod and apparatus for using blast-furnace slag in cement clinker production199642
JP H08143348 ACement composition—7
KR 970,008,685 B1Rapid hardening cement composition having high strength properties19975
KR 100,220,340 B1Quick-hardening cement composition and preparing method the same20007
KR 100,310,657 B1Quick-hardening cement composition having high solidity20017
US 5,494,515 C1Method and apparatus for using blast-furnace slag in cement clinker production200242
KR 100,670,458 B1The composition/Manufacturing/Process and Construction Method of the Dry Concrete for Repairing Concrete20073
JP 2007197286 AGrout composition, mortar or concrete using same and grouting material—9
KR 100,755,272 B1Early strength cement composition for latex-modified concrete200717
JP 2008179504 ABlast furnace slag cement—12
KR 20120050329 A환원 슬래그 분말을 이용한 초속경성 수경결합재 및 그 제조방법—13
US 8,834,625 B2Ultra-rapid hardening hydraulic binder using reduced slag powder, and method of preparing the same20142
US 8,986,444 B2Hybrid cement clinker and cement made from that clinker20154

Non-Patent Literature (4)

  • International Search Report(PCT/KR2012/010680), WIPO, dated Apr. 29, 2013.
  • JP 406321607 A (Tanaka et al.) Nov. 22, 1994 abstract.
  • JP 406321607 A (Tanaka et al.) Nov. 22, 1994 Machine Translation into English.
  • Korean Office Action(KR 10-2012-0081388), KIPO, dated Dec. 27, 2012.