Wafer with improved intrinsic gettering ability
Abstract
An integrated circuit with improved intrinsic gettering ability is described, having a bulk micro-defect (BMD) density of 3.85×105-3.38×109/cm3 through first and second annealing steps. The first annealing step is performed at a first temperature in an atmosphere containing at least one of oxygen gas and nitrogen gas. The second annealing step is performed at a second temperature higher than the first temperature in the atmosphere.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A wafer with improved intrinsic gettering ability, made from a Perfect Silicon wafer, and having a bulk micro-defect (BMD) density of 3.85×10 5 -3.38×10 9 /cm 3 through first and second annealing steps to the Perfect Silicon wafer, wherein the first annealing step is performed at a first temperature in an atmosphere containing at least one of oxygen gas and nitrogen gas, and the second annealing step is performed at a second temperature higher than the first temperature in the atmosphere.
- Claim 2Depends on #1
The wafer of claim 1 , which has a BMD density lower than 3.85×10 5 /cm 3 before the first and the second annealing steps.
- Claim 3Depends on #1
The wafer of claim 1 , wherein the first temperature is between 650° C. and 950° C. and the second temperature is between 1000° C. and 1200° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.