Patents
US 7,273,647 B2#13919745 Most CitedExpiredUnited States (USPTO)Utility

Silicon annealed wafer and silicon epitaxial wafer

8Forward Citations (#13919745 Global)
0.4/yrCitation Velocity (#19346297 Global)
1.47Citation PageRank (#23660183 Global)
7Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A silicon annealed wafer having a sufficient thick layer free from COP defects on the surface, and a sufficient uniform BMD density in the inside can be produced by annealing either a base material wafer having nitrogen at a concentration of less than 1×10 14 atoms/cm 3 , COP defects having a size of 0.1 μm or less in the highest frequency of occurrence and no COP defects having a size of 0.2 μm or more, oxygen precipitates at a density of 1×10 4 counts/cm 2 or more, and BMDs (oxygen precipitates), where the ratio of the maximum to the minimum of the BMD density in the radial direction of the wafer is 3 or less, or a base material wafer grown at specific average temperature gradients within specific temperature ranges and specific cooling times for a single crystal at a nitrogen concentration of less than 1×10 14 atoms/cm 3 , employing the Czochralski method. Moreover, a silicon epitaxial wafer having very small defects and a uniform BMD distribution in the inside can be formed by growing an epitaxial layer on the surface of either the first type base material wafer or the second type base material wafer. Both the silicon annealed wafer and the silicon epitaxial wafer greatly reduc

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A silicon annealed wafer, on the surface of which a COP defect free layer having a thickness of 5 μm or more is formed by annealing a base material wafer, wherein said base material wafer includes: a COP defect region of a single crystal containing nitrogen at a concentration of less than 1×10 14 atoms/cm 3 , wherein said COP defect has a size of 0.1 μm or less in the highest frequency of occurrence and there exist no COP defects having a size of more than 0.2 μm; oxygen precipitates formed at a density of 1×10 4 counts /cm 2 or more when said base material wafer is subjected to a oxygen pr

  2. Claim 2Depends on #1

    A silicon annealed wafer according to claim 1 , wherein the oxygen concentration of s