Patents
US 6,573,159 B1#2534263 Most CitedExpiredUnited States (USPTO)Utility

Method for thermally annealing silicon wafer and silicon wafer

28Forward Citations (#2534263 Global)
1.2/yrCitation Velocity (#4925340 Global)
4.42Citation PageRank (#4044287 Global)
24Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

According to the present invention, there are provided a method for heat treatment of silicon wafers wherein a silicon wafer is subjected to a heat treatment at a temperature of from 1000° C. to the melting point of silicon in an inert gas atmosphere, and temperature decreasing in the heat treatment is performed in an atmosphere containing 1-60% by volume of hydrogen, a method for heat treatment of silicon wafers under a reducing atmosphere containing hydrogen by using a rapid heating and rapid cooling apparatus, wherein temperature decreasing rate from the maximum temperature in the heat treatment to 700° C. is controlled to be 20° C./sec or less, and a silicon wafer which has a crystal defect density of 1.0×10 4 defects/cm 3 or more in a wafer bulk portion, a crystal defect density of 1.0×10 4 defects/cm 3 or less in a wafer surface layer of a depth of 0.5 μm from the surface, a crystal defect density of 0.15 defects/cm 2 or less on a wafer surface and surface roughness of 1.0 nm or less in terms of the P-V value. By these, crystal defects in wafer surface layers can be reduced by a simple method with a small amount of hydrogen used without degrading microroughness of wafers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 28.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for heat treatment of silicon wafers under a reducing atmosphere containing hydrogen by using a rapid heating and rapid cooling apparatus, wherein temperature decreasing rate from the maximum temperature in the heat treatment to 700° C. is controlled to be 20° C./sec or less.

  2. Claim 2Depends on #1

    The method for heat treatment of silicon wafers according to claim 1 , wherein the temperature decreasing rate in a region below 700° C. in the heat treatment is faster than the temperature decreasing rate from the maximum temperature to 700° C.

  3. Claim 3Depends on #1

    The method for heat treatment of silicon wafers according to claim 1 , wherein the reducing atmosphere containing hydrogen is 100% hydrogen or a mixed gas atmosphere of hydrogen with argon and/or nitrogen.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • S. Yamakawa et al., "Study of interface roughness dependence of electron mobility in Si inversion layers using the Monte Carlo method," American Institute of Physics, Jan. 1996, vol. 79, pp. 911-916.