Patents
US 8,093,165 B2#15531687 Most CitedActiveUnited States (USPTO)Utility

TiO2-containing silica glass and optical member for EUV lithography using the same

7Forward Citations (#15531687 Global)
0.5/yrCitation Velocity (#15522415 Global)
1.65Citation PageRank (#19788425 Global)
16Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a TiO 2 —SiO 2 glass in which when used as an optical member for an exposure tool for EUVL, a thermal expansion coefficient is substantially zero at the time of irradiation with high-EUV energy light, and physical properties of a multilayer can be kept over a long period of time by releasing hydrogen from the glass. The present invention relates to a TiO 2 -containing silica glass having a fictive temperature of 1,100° C. or lower, a hydrogen molecule concentration of 1×10 16 molecules/cm 3 or more, and a temperature, at which a linear thermal expansion coefficient is 0 ppb/° C., falling within the range of from 40 to 110° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A TiO 2 -containing silica glass having a TiO 2 content of at least 8% by mass, a fictive temperature of 1,100° C. or lower, a hydrogen molecule concentration of at least 1×10 17 molecules/cm 3 , an OH concentration of at least 600 ppm, temperature width in which a linear thermal expansion coefficient is 0±5 ppb/° C. (ΔT) of at least 8° C., and a temperature, at which a linear thermal expansion coefficient is 0 ppb/° C., falling within the range of from 40 to 110° C.

  2. Claim 2Depends on #1

    The TiO 2 -containing silica glass according to claim 1 , having a TiO 2 content of from 8 to 12% by mass.

  3. Claim 3Depends on #1

    The TiO 2 -containing silica glass according to claim 1 , having an average linear thermal expansion coefficient at from 20 to 100° C. of 60 ppb/° C. or lower.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Amendments submitted Oct. 28, 2010, in corresponding European Application No. 09714364.8, filed Feb. 27, 2009.
  • H. Oizumi et al., Japanese Journal of Applied Physics, vol. 46, No. 25, pp. L633-L635 (2007).
  • S. Graham et al. Proceedings of SPIE, vol. 5037, pp. 460-469 (2003).
  • U.S. Appl. No. 12/862,174, filed Aug. 24, 2010, Koike et al.
  • U.S. Appl. No. 12/868,900, filed Aug. 26, 2010, Koike et al.