Abstract
A method of making a silica glass having a uniform fictive temperature. The glass article is heated at a target fictive temperature, or heated or cooled at a rate that is less than the rate of change of the fictive temperature, for a time that is sufficient to allow the fictive temperature of the glass to come within 3° C. of the target fictive temperature. The silica glass is then cooled from the target fictive temperature to a temperature below the strain point of the glass at a cooling rate that is greater than the relaxation rate of the glass at the target fictive temperature. The silica glass has a fictive temperature that varies by less than 3° C. after the annealing step. A silica glass made by the method is also described.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of making a silica glass having a uniform fictive temperature, the method comprising the steps of: a. providing the silica glass, the silica glass having a strain point T s , a fictive temperature T f , and a relaxation rate at the fictive temperature T f , wherein the silica glass has a hydroxyl concentration that varies by at least 0.5 ppm; and b. annealing the silica glass, wherein annealing the silica glass comprises: i. heating the silica glass to a first temperature that is greater than target fictive temperature T f,t , cooling the glass to a second temperature that is less tha
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (1)
- U.S. Appl. No. 61/141,924, filed Dec. 31, 2008, Duran, Carlos et al.