Process for positive electrode active substance for lithium secondary battery
Abstract
A positive electrode active material for a lithium secondary battery containing a lithium-cobalt composite oxide is produced by firing, as a cobalt source, a mixture of substantially spherical cobalt hydroxide or tricobalt tetraoxide having such a sharp particle size distribution that the average particle size D50 is from 7 to 20 μm, and cobalt oxyhydroxide having an average particle size of secondary particles formed by agglomeration of primary particles of from 7 to 20 μm, in a proportion of from 5:1 to 1:5 as the cobalt atomic ratio, at a temperature of from 700° C. to 1050° C. in an oxygen-comprising atmosphere.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing a positive electrode active material, comprising: firing, as a cobalt source, a mixture of substantially spherical cobalt hydroxide or tricobalt tetraoxide having such a sharp particle size distribution that the average particle size D50 is from 7 to 20 μm, the average particle size D10 is at least 50% of the average particle size D50 and the average particle size D90 is at most 150% of the average particle size D50, and cobalt oxyhydroxide having an average particle size of secondary particles formed by agglomeration of primary particles of from 7 to 20 μm, in a propor
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (27)
Non-Patent Literature (3)
- IPDL JPO Machine Translation for JP 2003-257416.
- Machine Translation of JP-2002093417 (previously made of record by Applicant via IDS).
- U.S. Appl. No. 10/089,109, filed Mar. 26, 2002, Suhara, et al.