Patents
US 7,270,797 B2#17222122 Most CitedExpiredUnited States (USPTO)Utility

Process for producing positive electrode active material for lithium secondary battery

6Forward Citations (#17222122 Global)
0.3/yrCitation Velocity (#24890239 Global)
1.80Citation PageRank (#17129806 Global)
5Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

To provide a process for producing a lithium-cobalt composite oxide for a positive electrode of a lithium secondary battery excellent in volume capacity density, safety, charge and discharge cyclic durability, press density and productivity, by using in expensive cobalt hydroxide and lithium carbonate. A mixture having a cobalt hydroxide powder and a lithium carbonate powder mixed so that the atomic ratio of lithium/cobalt would be from 0.98 to 1.01, is fired in an oxygen-containing atmosphere at from 250 to 700° C., and the fired product is further fired in an oxygen-containing atmosphere at from 850 to 1,050° C., or such a mixture is heated at a temperature-raising rate of at most 4° C./min in a range from 250 to 600° C. and fired in an oxygen-containing atmosphere at from 850 to 1,050° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for producing a lithium-cobalt composite oxide for a positive electrode of a lithium secondary battery, comprising: forming a mixture of a cobalt hydroxide powder and a lithium carbonate powder so that an atomic ratio of lithium to cobalt is from 0.98 to 1.01; firing the mixture in an oxygen-containing atmosphere at a temperature of from 250 to 550° C. to obtain a fired product; and further firing the fired product in an oxygen-containing atmosphere at a temperature of from 850 to 1,050° C.; wherein the fired product is further fired without being pulverized.

  2. Claim 2Depends on #1

    The process according to claim 1 , wherein: in an X-ray diffraction spectrum of the cobalt hydroxide powder using Cu-Kα-ray, a half value width of a diffraction peak on (001)plane at 2θ=19±1° is from 0.18 to 0.35°, and a half value width of a diffraction peak on (101)plane at 2θ=38±1° i

Technical Overview & Description