Patents
US 6,929,883 B2#5114230 Most CitedExpiredUnited States (USPTO)Utility

Lithium-transition metal composite oxide

17Forward Citations (#5114230 Global)
0.8/yrCitation Velocity (#9034052 Global)
6.16Citation PageRank (#2361218 Global)
10Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a lithium-transition metal composite oxide having a large volume capacity density, high safety, excellent coating uniformity, excellent charge/discharge cycle durability and excellent low temperature characteristics, and suitable as a positive electrode active material for a lithium secondary cell. A lithium-transition metal composite oxide which is represented by the formula Li x M 1−y N y O 2 (wherein 0.2≦x≦1.2, 0≦y≦0.7, M is a transition metal element, and N is a transition metal element other than M or an alkaline earth metal element), wherein in the distribution curve of the cumulative volume particle size of said lithium composite oxide, the inclination of the curve at a cumulative volume fraction of 20% and 80% are at most 9%/μm and at least 3%/μm, respectively, and the average particle size is from 3 to 20 μm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 17.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A lithium-transition metal composite oxide which comprises particles of a lithium composite oxide represented by the formula Li x M 1−y N y O 2 , wherein 0.2≦x≦1.2, 0≦y≦0.7, M is a transition metal element, and N is a transition metal element other than M or an alkaline earth metal element, wherein in the distribution curve of the cumulative volume particle size of said lithium composite oxide, the inclination of the curve at a cumulative volume fraction of 20% is at most 9%/μm, the inclination of the curve at a cumulative volume fraction of 80% is at least 3%/μm, and the average particle size

  2. Claim 2Depends on #1

    The lithium-transition metal composite oxide according to claim 1 , wherein the cumulative volume fraction of particles having particle sizes of less than 1 μm, is at most 0.1%, and the cumulative volume fraction of particles having particle sizes of m

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 17 total)

PatentTitleYearCitations
US 8,173,301 B2Positive electrode active material for non-aqueous electrolyte secondary battery and non-aqueous electrolyte secondary battery including the same20123
US 2009017383 A1Positive electrode active substance for lithium secondary battery and process for producing the same—10
US 7,824,803 B2Positive electrode active substance for lithium secondary battery and process for producing the same20101
US 2013108921 A1Positive electrode active material for non-aqueous electrolyte secondary battery and production method for same, precursor for positive electrode active material, and non-aqueous electrolyte secondary battery using positive electrode active material—26
US 2011003204 A1Positive electrode for lithium secondary battery and lithium secondary battery comprising the same—1
US 8,758,652 B2Tungsten cathode material20140
US 2018076455 A1Positive electrode active material for non-aqueous electrolyte secondary battery and non-aqueous electrolyte secondary battery—1
US 9,553,311 B2Positive electrode active material for non-aqueous electrolyte secondary battery and production method for same, precursor for positive electrode active material, and non-aqueous electrolyte secondary battery using positive electrode active material20172
US 2005142444 A1Non-aqueous electrolyte secondary cell—13
US 7,981,547 B2Process for positive electrode active substance for lithium secondary battery20112
US 2010294985 A1Positive electrode active substance for lithium secondary battery and process for producing the same—6
US 2005170251 A1Positive electrode for lithium secondary battery and lithium secondary battery comprising the same—3
US 9,853,286 B2Positive electrode active material for non-aqueous electrolyte secondary battery and non-aqueous electrolyte secondary battery20172
US 11,588,153 B2Positive electrode active material for non-aqueous electrolyte secondary battery and non-aqueous electrolyte secondary battery20230
US 10,601,040 B2Positive electrode active material for non-aqueous electrolyte secondary battery and non-aqueous electrolyte secondary battery20201

Non-Patent Literature (5)

  • U.S. Appl. No. 10/089,109, filed Mar. 26, 2002, Suhara et al.
  • U.S. Appl. No. 10/296,205, filed Nov. 29, 2002, Suhara et al.
  • U.S. Appl. No. 10/743,479, filed Dec. 23, 2003, Suhara et al.
  • U.S. Appl. No. 10/849,856, filed May 21, 2004, Suhara et al.
  • U.S. Appl. No. 10/916,391, filed Aug. 12, 2004, Suhara et al.