Patents
US 4,152,181 A#7305567 Most CitedExpiredUnited States (USPTO)Utility

Cobalt alloy heat treatment

13Forward Citations (#7305567 Global)
0.3/yrCitation Velocity (#27052925 Global)
3.67Citation PageRank (#5474733 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A stabilization heat treatment for a class of wrought cobalt alloys is described. The heat treatment produces a useful combination of initial ductility, so as to permit fabrication of intricate parts, and adequate ductility even after long term exposure at elevated temperatures as, for example, that exposure encountered in gas turbine service. The heat treatment consists of a solution treatment performed at elevated temperatures followed by two aging steps at lower temperatures. The nominal alloy composition is 22.5% chromium, 4.25% aluminum, 15% (nickel+iron), 3% (tantalum+columbium), 10% (tungsten+molybdenum), 1.25% hafnium, 0.05% yttrium, 0.35% carbon, balance essentially cobalt.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of heat treating wrought cobalt alloys which contain about 18-25% chromium, about 3.7-4.6% aluminum, about 13-17% of a material selected from the group consisting of nickel and iron and mixtures thereof, about 2-4% of a material selected from the group consisting of tantalum and columbium and mixtures thereof, about 8-10% of a material selected from the group consisting of tungsten and molybdenum and mixtures thereof, about 0.5-2.0% hafnium, about 0.02-0.07% yttrium, about 0.25-0.45% carbon, balance essentially cobalt, said method comprising: (a) solution heat treating the alloy at a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗