US 4,581,913 A#1215668 Most CitedExpiredUnited States (USPTO)Utility

Method for improving the release and finish characteristics of metal stamping dies

43Forward Citations (#1215668 Global)
1.1/yrCitation Velocity (#5891384 Global)
9.36Citation PageRank (#1183220 Global)
16Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for improving the release and finish characteristics of metal stamping dies includes shot peening the interior die cavity walls with substantially spherical shot having a hardness value at least equal to the hardness value of the die cavity walls. Optimizing the parameters of the peening process, such as the Almen intensity and the shot type, size, hardness and uniformity, maximizes the improvement to the release and finish characteristics of the die. Optionally, the initial shot peening is followed by a second shot peening with substantially spherical glass beads. Metal stamping dies shot peened in accordance with the present method exhibit substantial improvement in their release and finish characteristics over unpeened dies.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 43.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for improving the release and finish characteristics of a metal stamping die formed of steel comprising shot peening the interior die cavity walls with substantially spherical shot having a hardness value at least equal to the hardness value of said die cavity walls, the peened die cavity walls being employed to directly contact metal work-pieces inserted in the die, without the die cavity walls being plated prior or subsequent to peening.

  2. Claim 2Depends on #1

    The method according to claim 1 wherein said shot comprises steel shot.

  3. Claim 3Depends on #2

    The method according to claim 2 wherein said steel shot has a Mil Spec size of from about SAE 70 to about SAE 230.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 43 total)

PatentTitleYearCitations
US 9,126,255 B2Press die for metal plate molding, the processing method of the surface of the press die, and manufacturing method of a vehicle body20151
US 7,703,312 B2Component with compressive residual stresses, process for producing and apparatus for generating compressive residual stresses201022
EP 0,612,585 A1Abrasive blasting apparatus and die finishing apparatus using the same—12
US 2008223099 A1Component With Compressive Residual Stresses, Process For Producing And Apparatus For Generating Compressive Residual Stresses—25
US RE46606 EStamping tool, casting mold and methods for structuring a surface of a work piece20170
US 4,944,172 AMethod of making a U-shaped closure tamper evident199038
US 7,066,234 B2Stamping tool, casting mold and methods for structuring a surface of a work piece200631
US 7,520,947 B2Cobalt alloys, methods of making cobalt alloys, and implants and articles of manufacture made therefrom200911
US 5,671,628 ALaser shock peened dies199726
US 9,415,433 B2Scrap shape retention20160
US 5,057,108 AMethod of surface finishing orthopedic implant devices1991142
US 2010135780 A1Component with Compressive Residual Stresses, Process for Producing and Apparatus for Generating Compressive Residual Stresses—7
US 5,193,375 AMethod for enhancing the wear performance and life characteristics of a brake drum199335
US 2012052194 A1Method of treating the surface of a cavity of a die used for casting—3
US 6,286,351 B1Tool engraving of a deformation tool for deforming with an active medium20016

Non-Patent Literature (4)

  • "Automatic Shot-Blasting of Hot Ingot Moulds", Process Control and Automation, vol. 10, Dec., 1963.
  • Automatic Shot Blasting of Hot Ingot Moulds , Process Control and Automation, vol. 10, Dec., 1963.
  • Woelfel and Mulhal, "Glass Bead Impact Blasting", Sep. 1982, vol. 122, No. 4, pp. 57-59.
  • Woelfel and Mulhal, Glass Bead Impact Blasting , Sep. 1982, vol. 122, No. 4, pp. 57 59.